Boron position-dependent surface reconstruction and electronic states of boron-doped diamond(111) surfaces - anab initiostudy
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2021-01-01 |
| Journal | Physical Chemistry Chemical Physics |
| Authors | Le The Anh, Francesca Celine I. Catalan, Yousoo Kim, Yasuaki Einaga, Yoshitaka Tateyama |
| Institutions | Keio University, National Institute for Materials Science |
| Citations | 10 |
Abstract
Section titled āAbstractāDependence of DOS on the boronās positions on a diamond(111) surface. In the bulk, boron interacts with carbon sp<sup>3</sup>and shows p-type characters. On the surface, boron strongly interacts with carbon sp<sup>2</sup>and exhibits surface states in the midgap.