Characterization of luminescence and electron transport in corroded zirconium alloys
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2021-01-01 |
| Journal | OSA Optical Sensors and Sensing Congress 2021 (AIS, FTS, HISE, SENSORS, ES) |
| Authors | Ricardo Vidrio, Maryam Zahedian, Hongliang Zhang, Bill Schneider, Xihong Zu |
| Institutions | University of WisconsinâMadison |
Abstract
Section titled âAbstractâNitrogen vacancy centers in diamond are used to image electron pathways in corroded zirconium alloys, with preliminary data showing unexpected luminescence from the oxidized zirconium. Our ongoing work includes identifying the origin of this luminescence.