Constructing a three-dimensional nano-crystalline diamond network within polymer composites for enhanced thermal conductivity

MetadataDetails
Publication Date2021-01-01
JournalNanoscale
AuthorsShaoyang Xiong, Yue Qin, Linhong Li, Guoyong Yang, Maohua Li
InstitutionsHangzhou Dianzi University, University of Chinese Academy of Sciences
Citations16

A facile and scalable method is developed to construct a three-dimensional porous diamond framework toward the high thermal conductivity of epoxy composites.