Diamond quantum sensors - from physics to applications on condensed matter research

MetadataDetails
Publication Date2021-01-02
JournalFunctional Diamond
AuthorsKin On Ho, Yang Shen, Yiu Yung Pang, Wai Kuen Leung, Nan Zhao
InstitutionsBeijing Computational Science Research Center, Chinese University of Hong Kong
Citations40

Single qubit in solid-state materials recently emerges as a versatile platform for quantum information. Among them, the nitrogen vacancy (NV) centre in diamond has become a powerful tool in quantum sensing for detecting various physics parameters, including electric and magnetic fields, temperature, force, strain, with ultimate precision and resolutions. It has been widely used in different conditions, from samples in ambient to samples in ultra-high pressure and low temperature. It can detect quantum phase transitions as well as neuron activities. Here we give a general review on both the physics of the sensing mechanism and protocols and applications.