Skip to content

Low-Temperature Spectroscopic Investigation of Lead-Vacancy Centers in Diamond Fabricated by High-Pressure and High-Temperature Treatment

MetadataDetails
Publication Date2021-09-15
JournalACS Photonics
AuthorsPeng Wang, Takashi Taniguchi, Yoshiyuki Miyamoto, Mutsuko Hatano, Takayuki Iwasaki
InstitutionsTokyo Institute of Technology, National Institute for Materials Science
Citations31

We report the optical observation of lead-vacancy (PbV) centers in diamond fabricated by Pb ion implantation and subsequent high-temperature annealing (2100 °C) under high pressure (7.7 GPa). Their optical properties were characterized by photoluminescence at varying temperatures down to 5.7 K. We observed intense emission peaks at 550 and 554 nm, with a large splitting of approximately 3900 GHz. The two lines are thought to correspond to the zero phonon line (ZPL) of PbV centers with split ground and excited states. A cubic trend of the ZPL width was observed while varying the temperature. We performed polarization measurements of the two lines in a single PbV center, showing nearly orthogonal dipole polarizations. These optical measurements strongly indicate that the PbV center possesses D3d symmetry in the diamond lattice. The observed large ground state splitting significantly suppresses the phonon-mediated transition, which causes decoherence of the electron spin state of the group IV color centers in diamond, leading to the expectation of a long spin coherence time at a temperature ∼9 K.