Electrochemical Ozone Generation Using Compacted High Pressure High Temperature Synthesized Boron Doped Diamond Microparticle Electrodes
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2021-12-01 |
| Journal | Journal of The Electrochemical Society |
| Authors | Georgia Wood, Irina M. Terrero RodrĂguez, Joshua J. Tully, Shayantan Chaudhuri, Julie V. Macpherson |
| Institutions | University of Warwick |
| Citations | 14 |
Abstract
Section titled âAbstractâElectrochemical ozone production (EOP) from water is an attractive, green technology for disinfection. Boron doped diamond (BDD) electrodes, grown by chemical vapor deposition (CVD), have been widely adopted for EOP due to their wide anodic window in water and excellent chemical and electrochemical stability. High pressure high temperature (HPHT) synthesis, an alternative growth technique used predominantly for the high-volume synthesis of nitrogen doped diamond microparticles, has been seldom employed for the production of conductive BDD electrodes. In this paper, we demonstrate, for the first time, the use of BDD electrodes fabricated from HPHT conductive BDD microparticles for EOP. The BDD microparticles are first compacted to produce freestanding solid electrodes and then laser micromachined to produce a perforated electrode. The compacted HPHT BDD microparticle electrodes are shown to exhibit high EOP, producing 2.23 ± 0.07 mg L â1 of ozone per ampere of current, at consistent levels for a continuous 20 h period with no drop off in performance. The HPHT electrodes also achieve a reasonable current efficiency of 23%, at a current density of 770 mA cm â2 .