A cascaded Brillouin laser using diamond Raman conversion

MetadataDetails
Publication Date2022-01-01
AuthorsHui Chen, Zhenxu Bai, Yunpeng Cai, Duo Jin, Richard P. Mildren
InstitutionsHebei University of Technology, Macquarie University

We demonstrate a diamond-based Brillouin laser with controllable, cascaded output spanning 15 cascaded SBS-Stokes-orders. Control of the cascading is achieved through both tailoring of the SBS cavity length and the SBS cavity output coupling.