Observation of high-order Laguerre-Gaussian beams from a diamond Raman laser
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2022-01-01 |
| Authors | Hui Chen, Yu Zhang, Hongwei Guo, Jiashuo An, Zhenxu Bai |
| Institutions | Hebei University of Technology |
Abstract
Section titled āAbstractāWe report on the direct generation of LG 0,m modes Stokes laser with m tunable range of 0-9, for the first time to our knowledge, in an external-cavity diamond Raman laser using Gaussian beam pumping.