Numerical Simulation of Orthogonal Machining of Gallium Nitride via Smoothed Particle Hydrodynamics
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2022-04-27 |
| Journal | NUML International Journal of Engineering and Computing |
| Authors | Muhammad Haseeb, Hasan Aftab Saeed, Imran S. S. Ghumman |
| Institutions | HITEC University, National University of Sciences and Technology |
Abstract
Section titled āAbstractāGallium Nitride is one of the best candidates for upcoming industrial revolution due to itssuperior electrical properties over silicon. In the present work, we investigate the chipformation, cutting force and effective stress in diamond machining of gallium nitride bysmoothed particle hydrodynamics approach based on Mohr-Coulomb material model. Thecomparison of the effective stress as reported by molecular dynamics studies and thatpredicted by the smoothed particle hydrodynamics simulation demonstrates the effectivenessof the smoothed particle hydrodynamics model.