Imaging of Magnitude and Phase of AC Magnetic Field Using Continuous-Wave Scheme with Diamond Sensor

MetadataDetails
Publication Date2022-07-31
AuthorsTakumi Mikawa, Karl J. Hallbäck, Yuichiro Matsuzaki, Yuta Nakano, Norio Tokuda
InstitutionsNational Institute of Advanced Industrial Science and Technology, The University of Tokyo

We successfully measured the mirometer-scale spatial-distribution of the magnitude and the phase of MHz-range AC magnetic field resonant to nitrogen-vacancy center in diamond by the continuous application of green laser and microwave.