Opportunities for nitrogen-vacancy-assisted magnetometry to study magnetism in 2D van der Waals magnets
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2022-08-08 |
| Journal | Applied Physics Letters |
| Authors | Abdelghani Laraoui, Kapildeb Ambal |
| Institutions | University of NebraskaāLincoln, Wichita State University |
| Citations | 20 |
Abstract
Section titled āAbstractāExploring and understanding magnetism in two-dimensional (2D) van der Waals (vdW) magnetic materials present a promising route for developing high-speed and low-power spintronics devices. Studying their magnetic properties at the nanoscale is challenging due to their low magnetic moment compared to bulk materials and the requirements of highly sensitive magnetic microscopy tools that work over a wide range of experimental conditions (e.g., temperature, magnetic field, and sample geometry). This Perspective reviews the applications of nitrogen-vacancy center (NV) based magnetometry to study magnetism in 2D vdW magnets. The topics discussed include the basics, advantages, challenges, and the usage of NV magnetometry.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2017 - Discovery of intrinsic ferromagnetism in two-dimensional van der Waals crystals [Crossref]
- 2017 - Layer-dependent ferromagnetism in a van der Waals crystal down to the monolayer limit [Crossref]
- 2019 - Two-dimensional magnetic crystals and emergent heterostructure devices [Crossref]
- 2019 - Van der Waals magnets: Wonder building blocks for two-dimensional spintronics? [Crossref]
- **** - Recent advances in two-dimensional magnets: Physics and devices towards spintronic applications [Crossref]
- 2020 - Recent advances in two-dimensional spintronics [Crossref]
- 2020 - Spintronics in two-dimensional materials [Crossref]
- 2016 - Magnetic anisotropy of the single-crystalline ferromagnetic insulator Cr2Ge2Te6 [Crossref]
- 2013 - Magnetic properties of layered itinerant electron ferromagnet Fe3GeTe2 [Crossref]
- 2018 - Electrical control of 2D magnetism in bilayer CrI3 [Crossref]