INVESTIGATION OF ISOTOPIC COMPOSITION AND PURITY OF 13C ENRICHED CVD-DIAMOND LAYERS BY RAMAN SPECTROSCOPY AND PHOTOLUMINESCENCE
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2022-11-16 |
| Journal | Journal of Applied Spectroscopy |
| Authors | Š. Š¢. Далказанов, M. O. Smirnova, Š”. Š. Š¢Š°ŃŠµŠ»ŠŗŠøŠ½, Š. Š”. ŠŃŃŠµŠ², Taisia Drozdova |
| Institutions | Technological Institute for Superhard and Novel Carbon Materials, National Academy of Sciences of Belarus |
Abstract
Section titled āAbstractāA method for estimating the isotopic composition and concentration of NV-centers in diamond using Raman scattering and photoluminescence spectra is presented. The proposed laboratory technique was used to study the spatial distribution of the 13C isotope and NV-centers in samples of CVD-diamond with isotopically
 modified layers.