STUDY ON THE INFLUENCE OF SINGLE CRYSTAL DIAMOND MATERIALS ON DETECTOR FABRICATION AND PERFORMANCE
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2023-01-01 |
| Journal | The Proceedings of the International Conference on Nuclear Engineering (ICONE) |
| Authors | Libin Wang, Yiyun Zhang, Guangwei Huang, Haijun Li, MA Zhihai |
| Institutions | Institute of Semiconductors, Chinese Academy of Sciences |
Abstract
Section titled āAbstractāSingle-crystal diamond (SCD), as an ultra-wide bandgap semiconductor material, has the advantages of high carrier mobility ,super radiation hardness characteristics, high thermal conductivity and high breakdown field intensity, making it an ideal material for the next generation of radiation detectors . The SCD film material is crucial to the radiation performance of the detectors, according to earlier investigations. In this paper, Metal-Semiconductor-Metal (MSM) SCD detectors were fabricated based on four different qualities SCD film materials manufactured by microwave plasma chemical vapor deposition (MPCVD) method, and their material characterization, electrical properties and radiation characteristics were examined. Atomic force microscopy (AFM), X-ray diffraction (XRD) and laser Raman scattering spectroscopy were used to analyze the surface morphology and lattice structure of several SCD films. The results of the characterization show that the two materials outperform the other two materials in terms of surface roughness and lattice defect density. The results indicated that the four detectors exhibited superior electrical properties, with resistivities over 1E13 Ω·cm, leakage currents below 2.5 pA at 100 V, and linear ohmic contact range of about ±0.3 V/μm. The charge collection efficiency and energy resolution of SCD detectors were measured by 238Pu α radioactive source. The charge collection efficiency of SCD detectors prepared by the two materials with better material characterization results was close to 100%, and the energy resolution was 2.5% and 2.1%, respectively Due to the considerable large surface roughness and many internal defects of the materials the other two detectors cannot be utilized for energy spectrum measurement, because of too small pulse amplitude and poor signal-to-noise ratio. Results can provide reference for selecting diamond film materials for radiation detectors and can be used to optimize the preparation process of diamond detectors.