Abstract
Section titled âAbstractâAbstract This study conducts a theoretical analysis on the stable structure, charge transfer, energy level transition, and electronic structure of a diamond yttrium vacancy color center. The color center in a diamond is very important as a single photon source material for quantum information processing technology and applications, such as temperature sensors, solid-state quantum systems, photonics, lighting, imaging technology, and biomedicine. Nanodiamond yttrium vacancy color centers are prepared using the solid substitution method with physical vapor deposition and microwave plasma chemical vapor deposition equipment. The density functional theory (DFT) is used to analyze the stability, electronic structure, and co-doping of N, Si, and O on the related defect structure of a rare Earth element yttrium-doped diamond using first-principle calculations, demonstrating consistency with the experimental results. The research shows that the fluorescence wavelength of an yttrium vacancy color center measured using the solid substitution method is 701.2 nm, which is located in the red region. The system is most stable when a Y atom replaces a carbon atom and there are two vacancies around it. The zero-phonon line of the diamond YV 2 defect is predicted to be 708.855 nm. Additionally, the influence doping is analyzed with N, Si, and O atoms. An yttrium-doped diamond emits light in the visible light region, which provides a theoretical basis for the application of diamond yttrium vacancy color centers.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2006 - Single defect centres in diamond: a review [Crossref]
- 2013 - Quantum measurement and entanglement of spin quantum bits in diamond [Crossref]
- 2018 - Germanium-vacancy color center in diamond as a temperature sensor [Crossref]
- 2019 - A diamond temperature sensor based on the energy level shift of nitrogen-vacancy color centers [Crossref]
- 2008 - Applied physics: diamond for quantum computing [Crossref]
- 2009 - Enhanced single-photon emission in the near infrared from a diamond color center [Crossref]
- 2008 - Diamond integrated quantum photonics [Crossref]
- 2011 - Creation and nature of optical centres in diamond for single-photon emission - overview and critical remarks [Crossref]
- 2017 - Synthesis of diamond in double carbon-rare Earth element systems [Crossref]