Skip to content

Microstructure and interface evolution of diamond/Cu composites prepared via ultrasonic additive manufacturing (UAM)

MetadataDetails
Publication Date2023-05-24
JournalJournal of Materials Research and Technology
AuthorsBo Wang, Fan Yang, Hongtao Zhang, Peng He
InstitutionsHarbin Institute of Technology
Citations13

Diamond-copper laminated composites with Cr-coating were prepared by ultrasonic additive manufacturing method. The microstructure and interfacial configuration between Cr-diamond and copper matrix were analyzed by scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), focused ion beam (FIB), and high-resolution transmission electron microscopy (HRTEM). Additionally, the microstructure evolution of the matrix around Cr-diamond particles were evaluated using electron backscatter diffraction (EBSD) method. The results reveal that the Cr-diamond achieves excellent solid bonding with the matrix due to violent plastic deformation. Moreover, we observe significant grain refinement and dynamic recrystallization at the interface of the matrix. The thermal conductivity of Dia/Cu composites is 428.07 ± 3.3W/mK and the diamond volume fraction is 8.8%.The study of this process can open up new avenues for low-temperature, low-pressure, free-design, and open fabrication of particle-reinforced metal matrix composites.

  1. 2005 - Metal matrix composites - from science to technological significance [Crossref]
  2. 2020 - Progress in research on hybrid metal matrix composites [Crossref]
  3. 2011 - Review of metal matrix composites with high thermal conductivity for thermal management applications [Crossref]
  4. 2019 - Effects of diamond particle size on the formation of copper matrix and the thermal transport properties in electrodeposited copper-diamond composite materials [Crossref]
  5. 2019 - Critical effect and enhanced thermal conductivity of Cu-diamond composites reinforced with various diamond prepared by composite electroplating [Crossref]
  6. 2020 - Research progress of diamond/copper composites with high thermal conductivity [Crossref]
  7. 2021 - High thermal conductive copper/diamond composites: state of the art [Crossref]
  8. 2021 - Manufacturing of complex diamond-based composite structures via laser powder-bed fusion
  9. 2019 - Microstructure of Cu-diamond composites with near-perfect interfaces prepared via electroplating and its thermal properties [Crossref]