Diamond Nanowire Piezoresistive Sensor Technical Documentation
Section titled “Diamond Nanowire Piezoresistive Sensor Technical Documentation”This document outlines key technical data regarding boron-doped diamond (BDD/UNCD) nanowire piezoresistive sensors (US Patent 9,441,940 B2) and explores how 6CCVD’s capabilities can address the engineering challenges of this technology.
Executive Summary
Section titled “Executive Summary”- Material Innovation: Piezoresistive pressure/strain sensors utilizing Boron-doped Ultra-NanoCrystalline Diamond (B-UNCD) nanowires.
- High Performance: Features a reported gauge factor of approximately 70-100 in B-UNCD nanowires, a key metric for strain sensitivity.
- Microfabrication Process: Nanowire fabrication on a silicon substrate using a sacrificial release method, enabling suspended structures for MEMS applications.
- Electrical Integration: B-UNCD nanowires anchored between Platinum/Gold contact pads to monitor resistance changes upon mechanical deflection.
- Protective Capping: The B-UNCD layer is encapsulated (e.g., with a thin oxide and polycrystalline diamond capping layer) to ensure structural integrity after release.
- Optical Compatibility: Diamond is highly transparent in the IR/visible spectra, enabling potential integration in optical sensing platforms.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Gauge Factor | 70 - 100 | unitless | Piezoresistive strain sensitivity |
| Dopant | Boron | - | p-type semiconductor dopant |
| Resistivity Target | 0.005 - 10 | Ω·cm | Tunable based on doping concentration |
| Substrate Material | Silicon | - | Sacrificial layer for nanowire release |
| Capping Layer | Polycrystalline Diamond | - | Encapsulation for nanowire protection |
| Active Layer Material | B-UNCD | - | Grain sizes typically 2 - 5 nm |
| Noble Metal Pads | Au / Pt | - | Contact metallization |
| Adhesion Layer | Ti / W | - | Common adhesion promoters for diamond |
(Note: Values consolidated from the methodology and prior art referenced in the patent. Specific parameters for individual devices can be tailored.)
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: A substrate (e.g., Silicon) is prepared featuring a sacrificial layer (e.g., SiO2) beneath the active diamond film.
- B-UNCD Growth: Chemical Vapor Deposition (CVD) is utilized to grow the boron-doped Ultra-NanoCrystalline Diamond film onto the substrate.
- Metallization Deposition: A metal stack (e.g., Ti / Pt / Au) is sputter-deposited or evaporated. Photolithography patterns the stack to define the contact pads.
- Masking: A dual masking layer (e.g., photoresist over hard mask) is applied and patterned to define the nanowire geometry.
- Reactive Ion Etching (RIE): Oxygen-based plasma etching transfers the mask pattern into the B-UNCD layer, carving out the free-standing nanowires.
- Release Process: A wet or vapor hydrofluoric acid (HF) etch selectively removes the underlying silicon dioxide sacrificial layer, leaving the B-UNCD nanowires suspended between anchor points.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”6CCVD provides the high-precision materials required to fabricate boron-doped diamond nanowire sensors and the engineering support to scale them into commercial MEMS devices.
- Applicable Materials: For strain gauge applications requiring high sensitivity, we recommend our Heavy Boron-Doped PCD (Polycrystalline Diamond). For researchers seeking more defined carrier mobility characteristics, our Optical Grade SCD (Single Crystal Diamond) can provide exceptional performance, though custom resistance tuning is required. The materials used in such nanowire transducers are closely related to our BDD (Boron-Doped Diamond) platform.
- Metallization Integration: 6CCVD provides in-house custom metalization services. We can deposit Ti, Pt, Au, W, and Pd adhesion and contact layers with high precision, ensuring robust ohmic contacts to diamond surfaces—an essential step for the piezoresistive functionality described in this patent.
- Customization Potential: We specialize in custom dimensions and laser cutting of diamond wafers up to 125mm (PCD) and thicknesses ranging from 0.1 µm to 500 µm. This ensures we can supply the exact thin-film substrates needed for microfabrication processes (e.g., LPCVD deposition, RIE etching) to engineer nanowire structures.
- Engineering Support: Our in-house engineering team, supported by PhD-level material scientists, is ready to consult on material selection for similar piezoresistive sensor projects. We assist clients in optimizing diamond grain size, doping uniformity, and surface morphology (polishing to Ra < 5nm for inch-size PCD) to maximize the gauge factor.
- Call to Action: For custom specifications, material consultation, or advanced prototyping of diamond-based sensors, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
A UNCD nanowire comprises a first end electrically coupled to a first contact pad which is disposed on a substrate. A second end is electrically coupled to a second contact pad also disposed on the substrate. The UNCD nanowire is doped with a dopant and disposed over the substrate. The UNCD nanowire is movable between a first configuration in which no force is exerted on the UNCD nanowire and a second configuration in which the UNCD nanowire bends about the first end and the second end in response to a force. The UNCD nanowire has a first resistance in the first configuration and a second resistance in the second configuration which is different from the first resistance. The UNCD nanowire is structured to have a gauge factor of at least about 70, for example, in the range of about 70 to about 1,800.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”- DOI: None