Effects of oxygen/nitrogen co-incorporation on regulation of growth and properties of boron-doped diamond films
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2023-07-06 |
| Journal | Chinese Physics B |
| Authors | Dong-Yang 东阳 Liu 刘, Kun 琨 Tang 汤, Shun-Ming 顺明 Zhu 朱, Rong 荣 Zhang 张, You-Dou 有炓 Zheng 郑 |
| Institutions | Nanjing University |
| Citations | 4 |
Abstract
Section titled “Abstract”Regulation with nitrogen and oxygen co-doping on growth and properties of boron doped diamond films is studied by using laughing gas as dopant. As the concentration of laughing gas (N 2 O/C) increases from 0 to 10%, the growth rate of diamond film decreases gradually, and the nitrogen-vacancy (NV) center luminescence intensity increases first and then weakens. The results show that oxygen in laughing gas has a strong inhibitory effect on formation of NV centers, and the inhibitory effect would be stronger as the concentration of laughing gas increases. As a result, the film growth rate and nitrogen-related compensation donor decrease, beneficial to increase the acceptor concentration (∼3.2 × 10 19 cm −3 ) in the film. Moreover, it is found that the optimal regulation with the quality and electrical properties of boron doped diamond films could be realized by adding appropriate laughing gas, especially the hole mobility (∼700 cm 2 /V⋅s), which is beneficial to the realization of high-quality boron doped diamond films and high-level optoelectronic device applications in the future.