Diamond dielectric characterization with superconducting LC micro-resonators
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2023-09-17 |
| Authors | F. Mazzocchi, D. StrauĂ, T. Scherer |
| Institutions | Karlsruhe Institute of Technology |
Abstract
Section titled âAbstractâIn this work we present a study evaluating superconducting LC micro-resonators as potentially useful characterization tools for dielectric materials, with a particular focus on poly-and single crystalline diamond substrates.