Efficient extraction of zero-phonon-line photons from single nitrogen vacancy centers in an integrated GaP-on-diamond platform

MetadataDetails
Publication Date2016-01-01
AuthorsEmma Schmidgall, Michael N. Gould, Shabnam Dadgostar, Fariba Hatami, Kai‐Mei C. Fu
InstitutionsUniversity of Washington, Humboldt-Universität zu Berlin
Citations5

We demonstrate optical coupling of single NV center zero phonon emission to integrated GaP-on-diamond waveguides, with estimated total quantum efficiency values above 10% due to Purcell enhancement and efficient coupling between the cavities and waveguides.