Oxidation of Formaldehyde on PdNi Nanowires Synthesized in Superfluid Helium
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2023-10-01 |
| Journal | Электрохимия |
| Authors | Roman A. Manzhos, V. K. Kochergin, А. Г. Кривенко, I. I. Khodos, A. V. Karabulin |
| Institutions | Joint Institute for High Temperatures, Semenov Institute of Chemical Physics |
Abstract
Section titled “Abstract”The possibility of using a boron-doped diamond electrode with a net structure of PdNi alloy nanowires deposited on its surface by laser ablation in superfluid helium as a formaldehyde sensor is considered. High sensitivity of such an electrode to trace amounts of formaldehyde was shown.