Measurement of Two-Photon Absorption Coefficient of 1030 nm Ultrashort Laser Pulses on Natural Diamond Color Centers
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2023-10-01 |
| Journal | Optics and Spectroscopy |
| Authors | Yulia Gulina |
| Institutions | P.N. Lebedev Physical Institute of the Russian Academy of Sciences |
Abstract
Section titled āAbstractāAn experimental study of nonlinear absorption process of ultrashort laser pulses in bulk of natural diamond has been carried out. The results of experimental studies on measuring nonlinear transmission of 1 mm thick plane-parallel plate made of diamond irradiated with focused by micro lens (NA = 0.55 with focal length f ā = 5 mm) 0.3 and 10 ps laser pulses with 1030 nm wavelength are presented. It is shown that in this sample the main attenuation mechanism of ultrashort laser pulses with 1030 nm wavelength at intensities not exceeding 10 TW/cm2 is two-photon absorption at color centers, the absorption coefficient β2 = 4.1 ± 0.3 cm/TW is determined.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2013 - Ultrafast nonlinear optics [Crossref]