Single spin magnetometry and relaxometry applied to antiferromagnetic materials

MetadataDetails
Publication Date2023-10-01
JournalAPL Materials
AuthorsAurore Finco, V. Jacques
InstitutionsUniversitƩ de Montpellier, Laboratoire Charles Coulomb
Citations12

Despite the considerable interest for antiferromagnets that appeared with the perspective of using them for spintronics, their experimental study, including the imaging of antiferromagnetic textures, remains a challenge. To address this issue, quantum sensors, and, in particular, the nitrogen-vacancy (NV) defects in diamond have become a widespread technical solution. We review here the recent applications of single NV centers to study a large variety of antiferromagnetic materials, from quantitative imaging of antiferromagnetic domains and non-collinear states, to the detection of spin waves confined in antiferromagnetic textures and the non-perturbative measurement of spin transport properties. We conclude with recent developments improving further the magnetic sensitivity of scanning NV microscopy, opening the way to detailed investigations of the internal texture of antiferromagnetic objects.

  1. 2020 - Seeing is believing: Visualization of antiferromagnetic domains [Crossref]
  2. 2016 - Antiferromagnetic spintronics [Crossref]
  3. 2018 - Antiferromagnetic spintronics [Crossref]
  4. 1960 - Neutron and optical studies of domains in NiO [Crossref]
  5. 1993 - Spontaneous non-reciprocal reflection of light from antiferromagnetic Cr2O3 [Crossref]
  6. 1995 - Domain topography of antiferromagnetic Cr2O3 by second-harmonic generation [Crossref]
  7. 2001 - Nonreciprocal magnetic photonic crystals [Crossref]
  8. 2018 - Observation of magnetic vortex pairs at room temperature in a planar α-Fe2O3/Co heterostructure [Crossref]
  9. 2006 - Atomic spin structure of antiferromagnetic domain walls [Crossref]
  10. 2007 - Magnetic exchange force microscopy with atomic resolution [Crossref]