Investigation of the moisture classification and moisture removal behavior of diamond wire saw silicon powder waste cake

MetadataDetails
Publication Date2023-12-14
JournalJournal of Materials Research and Technology
AuthorsShifeng Han, Shicong Yang, Kuixian Wei, Wenhui Ma
Citations18

When processing silicon wafers for photovoltaic power generation, approximately 35 % of high-purity silicon is lost as a diamond wire saw silicon powder (DWSSP) waste cake with a high moisture content. The high moisture content of DWSSP results in the oxidation of high-purity silicon, which hinders the recovery and utilization of silicon resources. Disappointingly, a method for the removal of moisture from the DWSSP waste cake, which is crucial for silicon recovery, has not yet been revealed. In the present study, a novel investigation was conducted to determine the moisture classification of a DWSSP waste cake and to reveal the moisture removal behavior. The results indicate that the moisture content in the DWSSP waste cake can be divided into two distinct categories: surface adsorbed water and capillary water. Moreover, the kinetics analysis and simulation demonstrated that the elimination of moisture predominantly takes place during the constant-rate period and the falling-rate period. Increasing the drying temperature and reducing the equivalent diameter of the DWSSP waste cake will contribute to improving the efficiency of moisture removal. The application of the findings of this study can help to reduce the harmful environmental impacts of DWSSP and achieve the efficient recovery of silicon resources.

  1. 2020 - New insights into the solid-state hydrogen storage of nanostructured LiBH4-MgH2 system [Crossref]
  2. 2022 - A novel approach for simultaneous recycling of Ti-bearing blast furnace slag, diamond wire saw Si powder, and Al alloy scrap for preparing TiSi2 and Al-Si alloys [Crossref]
  3. 2023 - MXene-decorated bio-based porous carbon composite phase change material for superior solar-thermal energy storage and thermal management of electronic components [Crossref]
  4. 2023 - Recent advances in kinetic and thermodynamic regulation of magnesium hydride for hydrogen storage [Crossref]
  5. 2020 - Mechanism of enhancing Fe removal from metallurgical grade silicon by metal-assisted chemical leaching [Crossref]
  6. 2018 - Electrodeposition and characterization of Cu2O thin films using sodium thiosulfate as an additive for photovoltaic solar cells, Chin
  7. 2021 - Influence of iron, aluminum, calcium, titanium and vanadium impurities removal from silicon based on Cu-catalyzed chemical leaching [Crossref]
  8. 2012 - Boron removal from metallurgical-grade silicon using lithium containing slag [Crossref]
  9. 2023 - Failure mechanism of parallel gap resistance welding joint between Ag foil and GaAs solar cell by temperature cycling [Crossref]
  10. 2021 - Silicon recovery from diamond wire saw silicon powder waste with hydrochloric acid pretreatment: an investigation of Al dissolution behavior [Crossref]