(Invited) Leading-Edge Diamond FET, MEMS, and Photodetector Devices
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2023-12-22 |
| Journal | ECS Meeting Abstracts |
| Authors | Yasuo Koide |
| Institutions | National Institute for Materials Science |
Abstract
Section titled âAbstractâDiamond is a candidate material for next-generation power electronics, micro-electro mechanical systems (MEMS), and solar-blind deep-ultraviolet (DUV) photodetector devices with excellent thermal stability and radiation hardness, which operate under extreme environment. In order to use an advantage of high-density hole channel of hydrogenated diamond (H-diamond) surface, we have developed the high-k stack gate dielectrics and AlN heterojuction gate for H-diamond FETs, such as HfO 2 /HfO 2 , LaAlO 3 /Al 2 O 3 Ta 2 O 5 /Al 2 O 3 , and ZrO 2 /Al 2 O 3 , AlN/Al 2 O 3 prepared by a combination of sputter-deposition (SD) and atomic layer deposition (ALD) techniques [1,2]. We also demonstrated the artificial diamond Fin-FETs with high-current level [3] and the nanolaminate insulator gate metal-oxide-gate FETs (MOSFETs) with k value as high as 100 [4], and the new transistor concept named by metal-insulator-metal-semiconductor field-effect transistor (MIMS-FET) to achieve normally-off operation by combining the advantages of MOSFET and metal-semiconductor FET [5]. In addition, we developed the routine ion-implantation process for preparing the diamond cantilever with a resonant frequency quality factor as high as one million [6,7]. We have also developed thermally stable Schottky barrier photodiode (SPD), metal-semiconductor-metal photodetector (MSMPD), and MSM-type SPD (IDF-SPD) with a large photoconductivity gain in DUV wavelength and a large discrimination ratio between DUV/visible light responsivity [8,9]. In this presentation, we will review the comprehensive our work on the diamond FET, MEMS, and photodetector devices. Acknowledgements : This work was in collaboration with J-W. Liu, M. Imura, M-Y. Liao, J. Alvarez in NIMS and A. Ouchiero and E. Obaldia in University of Taxes, Dallas, and partly supported by JSPS KAKENHI Grant Number 20H00313. References [1] Liu, M-Y. Liao, M. Imura, A. Tanaka, H. Iwai, Y. Koide, âLow on-resistance diamond field effect transistor with high-k ZrO 2 as dielectric,â Sci. Reports, vol. 4, 6395-1 (2014). [2] Liu and Y. Koide, âAn overview of high-k oxides on hydrogenated-diamond for metal-oxide-semiconductor capacitors and field-effect transistors.â SENSORS, 18, No.6, 813 (2018). [3] Liu, H. Ohsato, Bo Da, Y. Koide, âHigh Current Output Hydrogenated Diamond Triple-Gate MOSFETs,â IEEE J. Electron Devices Society. 7, 561 (2019). [4] Liu, O. Auciello, E. de Obaldia, B. Da, Y. Koide, âScience and Technology of Integrated Super-High Dielectric Constant AlOx/TiOy Nanolaminates / Diamond for MOS Capacitors and MOSFETs,â Carbon. 172 112 (2021). [5] Liao, L. Sang, T. Shimaoka, M. Imura, S. Koizumi, Y. Koide, âEnergyâEfficient Metal-Insulator-MetalâSemiconductor FieldâEffect Transistors Based on 2D Carrier Gases,â Advanced Electronic Materials. 5 [5] (2019). [6] Liao, S. Hishita, E. Watanabe, S. Koizumi, Y. Koide, âSuspended single-crystal diamond nanowires for high-performance nanoelectro- mechanical switches.â Adv. Mater. 22, 5393 (2010). [7] Wu, L. Sang, T. Teraji, T. Li, K. Wu, M. Imura, J. You, Y. Koide, M. Liao, âReducing energy dissipation and surface effect of diamond nanoelectromechanical resonators by annealing in oxygen ambient,â Carbon. 124, 281 (2017). [8] M. Liao, Y. Koide, and J. Alvarez, âThermally Stable visible-blind Diamond Photodiode Using WC Schottky Contact,â Appl. Phys. Lett ., 87, p. 0221051 (2005). [9] Liao and Y. Koide, âHigh-performance metal-semiconductor-metal deep-ultraviolet photodetectors based on homoepitaxial diamond thin film.â Appl. Phys. Lett. 89, 113509 (2006).