Wear of Carbide Plates with Diamond-like and Micro-Nano Polycrystalline Diamond Coatings during Interrupted Cutting of Composite Alloy Al/SiC
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2023-12-08 |
| Journal | Journal of Manufacturing and Materials Processing |
| Authors | E. E. Ashkinazi, Sergey V. Fedorov, Artem Martyanov, Vadim Sedov, R. A. Khmelnitsky |
| Institutions | P.N. Lebedev Physical Institute of the Russian Academy of Sciences, Moscow State Technological University |
| Citations | 2 |
| Analysis | Full AI Review Included |
ERROR: File too large (11.3MB)
View Original Abstract
The complexity of milling metal matrix composite alloys based on aluminum like Al/SiC is due to their low melting point and high abrasive ability, which causes increased wear of carbide tools. One of the effective ways to improve its reliability and service life is to modify the surface by plasma chemical deposition of carbon-based multilayer functional layers from vapor (CVD) with high hardness and thermal conductivity: diamond-like (DLC) or polycrystalline diamond (PCD) coatings. Experiments on an indexable mill with CoroMill 200 inserts have shown that initial tool life increases up to 100% for cases with DLC and up to 300% for multilayered MCD/NCD films at a cutting speed of 800 m/min. The primary mechanism of wear of a carbide tool in this cutting mode was soft abrasion, when wear on both the rake and flank surfaces occurred due to the extrusion of cobalt binder between tungsten carbide grains, followed by their loss. Analysis of the wear pattern of plates with DLC and MCD/NCD coatings showed that abrasive wear begins to prevail against the background of soft abrasion. Adhesive wear is also present to a lesser extent, but there is no chipping of the base material from the cutting edge.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2022 - Fabrication, microstructure, and machinability of aluminum metal-matrix composites
- 2023 - A Systematic Review on the Mechanical, Tribological, and Corrosion Properties of Al 7075 Metal Matrix Composites Fabricated through Stir Casting Process
- 2016 - Studies on Mechanical Properties of Al-SiC Metal Matrix Composite
- 2016 - Mechanical and Tribological Properties of Centrifugally Cast Al-Si-SiC Composites
- 2016 - Effects of SiCp Reinforcement on the Abrasive Wear Properties of Al-Si Alloy [Crossref]
- 2016 - Machining of aluminum alloys: A review [Crossref]
- 2017 - Machinability and Wear of Aluminium Based Metal Matrix Composites by MQLâA Review [Crossref]
- 2023 - Study of tool flank wear and surface quality in milling of Al520-MMCs reinforced with SiC and Sn particles