Optical and Spin Coherence of NV centers in Isotopically Purified Diamond for Quantum Networks

MetadataDetails
Publication Date2024-01-01
JournalQuantum 2.0 Conference and Exhibition
AuthorsHendrik B. van Ommen, Kai-Niklas Schymik, T. Yamamoto, T. H. Taminiau

We discuss measurements on single NV centers in isotopically purified diamond and show coherent optical transitions combined with enhanced electron and carbon spin coherence. These results open avenues for new quantum network applications.