Towards Quantum Resolution Limit of Magnetic Field Imaging with Nitrogen-Vacancy Centers
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2024-01-01 |
| Authors | Nico Deshler, Ayan Majumder, Kasturi Saha, Saikat Guha |
Abstract
Section titled āAbstractāNitrogen-vacancy centers are an emerging platform for optically interrogating spatially-varying magnetic fields. We calculate the quantum Fisher information matrix pertaining to the positions and local magnetic fields of two nitrogen-vacancy centers under the ODMR protocol.