Abstract
Section titled âAbstractâ<p>In this work, four different techniques were concurrently applied to study the interplay between local electroactivity and electrode surface characteristics of free-standing, polycrystalline boron-doped diamond (BDD). Scanning electron microscopy, electron back-scatter diffraction, Raman mapping and scanning electrochemical microscopy were used to probe the electrode morphology, grain orientation and boundaries, composition, and local electrochemical activity, respectively. Both nucleation and growth BDD surfaces together with the cross-section area were carefully investigated for the first time in a single study using the combination of all four techniques. This enabled us to obtain significant insights into the highly heterogeneous nature of the polycrystalline BDD material. Notably, boron dopants were confirmed to be non-uniformly distributed over the BDD material, which is characterized by a distinct columnar structure and composition of grains of various orientations. Particularly, the highest electrochemical activity was recorded on the highest doped (111) crystal orientation. In contrast, the averagely boron-doped (100)-oriented facet showed non-conductive nature. This highlights that the local electrochemical activity of the BDD surface is strongly grain-dependent and the most significant factors governing the obtained responses are crystallographic orientation and boron doping. Moreover, increased boron and sp<sup>2</sup> carbon content in the boundary regions was recognized by Raman mapping. However, such localized enrichment in impurities did not translate into enhanced electrochemical activity, which implies that boron atoms at the inter-grain areas are predominantly inactive. Finally, it is crucial to consider all characteristics of the polycrystalline BDD including crystal orientation, which is particularly relevant if micro- and nanoscale probing is intended.</p>
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2019 - Recent progress in the applications of boron doped diamond electrodes in electroanalysis of organic compounds and biomolecules - A review [Crossref]
- 2022 - Boron-doped diamond electrodes: Recent developments and advances in view of electrochemical drug sensors [Crossref]
- 2022 - Boron-doped diamond electrode outperforms the state-of-the-art electrochemiluminescence from microbeads immunoassay [Crossref]
- 2019 - Recent developments and advances in boron-doped diamond electrodes for electrochemical oxidation of organic pollutants [Crossref]
- 2020 - Characterization of the reaction environment in flow reactors fitted with BDD electrodes for use in electrochemical advanced oxidation processes: A critical review [Crossref]
- 2022 - Experimental insights into anodic oxidation of hexafluoropropylene oxide dimer acid (GenX) on boron-doped diamond anodes [Crossref]
- 2019 - Use of boron-doped diamond electrodes in electro-organic synthesis [Crossref]
- 2021 - Photoelectrocatalytic interface of boron-doped diamond: Modification, functionalization and environmental applications [Crossref]
- 2021 - Diamond supercapacitors: Progress and perspectives [Crossref]
- 2019 - Conductive diamond: synthesis, properties, and electrochemical applications [Crossref]