We present site-coincident imaging of a high dislocation density boron-doped chemical vapor deposition-grown homoepitaxial (001) diamond film using electron channeling contrast imaging (ECCI), cathodoluminescence, transmission electron microscopy (TEM), and scanning secondary ion mass spectroscopy (SIMS). With growing interest in large area heteroepitaxial substrates, we show that ECCI is a promising technique to accurately evaluate dislocations in diamond films. We find the electron backscatter yield is sufficient to distinguish individual threading dislocations in ECCI despite the low atomic number of carbon, and we have generally good agreement between dislocations observed in ECCI and TEM of the same region. Importantly, relying on luminescence in the 430 nm dislocation-related A-band alone results in an underestimation of the defect density as we find only 20%-40% of the threading dislocations luminesce. We further show that dislocations do not perturb the spatial uniformity of boron doping measured by SIMS, even when the dislocations are clustered with high density, and we can tentatively rule out strong segregation effects at the dislocations. Our results establish the complementary use of microscopy and microanalysis methods to rapidly characterize and understand the impact of dislocations in diamond thin films.

  1. 2020 - Diamond power devices: State of the art, modelling, figures of merit and future perspective [Crossref]
  2. 2021 - Materials challenges for quantum technologies based on color centers in diamond [Crossref]
  3. 2013 - Diamond NV centers for quantum computing and quantum networks [Crossref]
  4. 2021 - Recent progress in diamond radiation detectors [Crossref]
  5. 2014 - Diamond for particle and photon detection in extreme conditions [Crossref]
  6. 2010 - Diamond detectors for hadron physics research [Crossref]
  7. 2020 - High yield uniformity in pseudo-vertical diamond Schottky barrier diodes fabricated on half-inch single-crystal wafers [Crossref]
  8. 2005 - Free-standing diamond single crystal film for electronics applications [Crossref]
  9. 2019 - Imaging crystal stress in diamond using ensembles of nitrogen-vacancy centers [Crossref]
  10. 2017 - Characteristic luminescence correlated with leaky diamond Schottky barrier diodes [Crossref]