Near zero-field microwave-free magnetometry with ensembles of nitrogen-vacancy centers in diamond

MetadataDetails
Publication Date2024-06-11
JournalPhysical review. B./Physical review. B
AuthorsOmkar Dhungel, T. Lenz, Muhib Omar, Joseph Shaji Rebeirro, Minh-Tuan Luu
InstitutionsLinkƶping University, Helmholtz Institute Mainz
Citations7

<p>Abstract:</p> <p>We study cross-relaxation features near zero magnetic field with ensembles of nitrogen-vacancy (NV) centers in diamond and examine their properties in samples with a range of 0.9–16.0 ppm of NV concentrations. The observed NV-NV cross-relaxation features between differently oriented NV centers in high (≳0.9 ppm)-NV-density samples hold promise for a variety of magnetometry applications where microwave fields (or any bias field) disturb the system under study. We theoretically determine the values of the bias magnetic fields corresponding to cross relaxations between different axes and experimentally validate them. The behavior of zero-field cross-relaxation features as a function of temperature is also investigated.</p>