Skip to content

Thermal annealing of radiation damages produced by swift 14N and 16O ions in LiF crystals

MetadataDetails
Publication Date2024-06-20
JournalMaterials Research Express
AuthorsМ. Š’. Дорокин, Zh B Malikova, Alma Dauletbekova, Guldar Baubekova, Gulnara Aralbayeva
Citations5

Abstract Annealing of color centers was studied in lithium fluoride crystals, irradiated with 23-MeV nitrogen and 28-MeV oxygen ions. Basing on the optical absorption spectroscopy and reaction-rate modelling, a new interpretation of the annealing kinetics at the practically important temperatures below 500 K is suggested. Proposed model explains simultaneous decrease of the F and F 2 /F 3 + peaks as a result of migration of the F centers and formation of larger aggregates, and does not include additional assumptions about impurities and cation vacancies. It specifies the migration energy of the F centers in the ground state to be about 1.3 eV, that corresponds to earlier studies.

  1. 2005 - Swift heavy ion induced structural and optical modifications in LiF thin film [Crossref]
  2. 1972 - Defect Creation by Radiation in Polar Crystals. [Crossref]
  3. 2008 - Effect of electronic energy loss and irradiation temperature on color-center creation in LiF and NaCl crystals irradiated with swift heavy ions [Crossref]
  4. 1998 - Chemical etching of ion tracks in LiF crystals [Crossref]
  5. 2000 - Theory of the late stage of radiolysis of alkali halides [Crossref]
  6. 2012 - Color centers and structural damage in LiF induced by 150 MeV Kr ions [Crossref]
  7. 2008 - Stabilization and annealing of interstitials formed by radiation in binary metal oxides and fluorides [Crossref]
  8. 2023 - Molecular ion desorption from LiF(110) surfaces by positron annihilation [Crossref]
  9. 2020 - Distribution of color centers around swift ion trajectories in lithium fluoride crystals
  10. 2002 - Ion tracks on LiF and CaF2 single crystals characterized by scanning force microscopy