Tracking single charge jumping with an individual color center in diamond
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2024-06-05 |
| Journal | Physical review. B./Physical review. B |
| Authors | Chong-Jun Weng, Shujie Lin, Jiaxi Zhao, Yu Yang, Mingxue Cai |
| Institutions | University of Science and Technology of China, Chinese Academy of Sciences |
| Citations | 2 |
Abstract
Section titled āAbstractāAcquiring knowledge about the internal field environment of a solid-state spin is essential for its effective utilization as an external field detector. Working with the nitrogen-vacancy (NV) center in our diamond sample, we observed that almost all the NV centers with high effective field near the diamond surface has two sets of ODMR which we refer to as two states. Remarkably, near room temperature, these NV centers can spontaneously transition between these two states. Our experiments demonstrate that for NV centers with high ODMR splitting and shifting, the effective field cannot be solely attributed to a pure electric field. By sweeping the polarization direction of the microwave (MW) driving field, we extract both the strength and direction of the effective field. Furthermore, we track the real-time behavior of charges within the diamond by monitoring alternations in the Rabi frequencies, providing deeper insight into their hopping dynamics. These findings suggest the potential for manipulating NV centers by regulating the surrounding charge environment.