(C<sub>4</sub>H<sub>9</sub>)<sub>3</sub>CH<sub>3</sub>NBF<sub>4</sub>–С<sub>nanodiamonds</sub>
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2024-07-12 |
| Journal | Электрохимия |
| Authors | I. A. Stebnitsky, Н. Ф. Уваров, Yu. G. Mateyshina |
| Institutions | Institute of Solid State Chemistry and Mechanochemistry, Novosibirsk State University |
Abstract
Section titled “Abstract”The paper presents the results of studies of the structural, thermal and transport properties of solid composite electrolytes (1 - x)(C4H9)3CH3NBF4 - xCND (where CND are nanosized diamonds, 0 ≤ x 1, x is the mole fraction). It has been shown by the Powley method that the crystal structure of the low-temperature phase (C4H9)3CH3NBF4 is described by the space symmetry group P42/ncm. It was found that the addition of a nanodiamond inert additive leads to an increase in the electrical conductivity of the composite electrolyte by 4 orders of magnitude up to a value of 1.3∙10-3 S/cm at 145°C at x = 0.98. The theoretical dependences describe well the experimental data in the concentration range 0 ≤ x ≤ 0.99 at temperatures of 84 and 127 оC.