Lossless Phonon Transition Through GaN‐Diamond and Si‐Diamond Interfaces
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2024-07-08 |
| Journal | Advanced Electronic Materials |
| Authors | Mohamadali Malakoutian, Kelly Woo, D. Rich, Ramandeep Mandia, Xiang Zheng |
| Institutions | University of Maryland, College Park, Arizona State University |
| Citations | 21 |
Abstract
Section titled “Abstract”Abstract Advancing Silicon (Si) technology beyond Moore’s law through 3D architectures requires highly efficient heat management methods compatible with foundry processes. While continued increases in transistor density can be achieved through 3D architectures, self‐heating in the upper tiers degrades the performance. Self‐heating is a critical problem for high‐power, high‐frequency, wide bandgap, and ultra‐wide bandgap devices as well. Diamond, known for its exceptional thermal conductivity, offers a viable solution in both these cases. Since thermal boundary resistance (between the channel/junction and diamond plays a crucial role in overall thermal resistance, this study investigates various dielectrics for interface engineering, such as Silicon dioxide (SiO 2 ), amorphous‐ Silicon Carbide (a‐SiC), and Silicon Nitride (SiN x ), to make a phonon bridge at gallium nitride (GaN)‐diamond and Si‐diamond interfaces. The a‐SiC interlayer reduces diamond/GaN (<5 m 2 K per GW) and diamond/Si (<2 m 2 K per GW) thermal boundary resistances by linking low‐ and high‐frequency phonons, boosting phonon transport through the interface. Engineered interfaces enhance heat spreading from the channel/junction and rule out premature failure.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2022 - Techcon 2022