Protocol for the preparation of TiO2-modified boron-doped diamond photoelectrode via electrophoretic deposition and its photoelectrochemical study

MetadataDetails
Publication Date2024-08-10
JournalSTAR Protocols
AuthorsWendy Quilumbaquin, G. Xavier Castillo-Cabrera, Luis J. Borrero-GonzƔlez, Patricio J. Espinoza-Montero
InstitutionsPontificia Universidad Católica del Ecuador
Citations3

Electrophoretic deposition is a straightforward method for synthesizing high-quality photoanodes. We present a protocol for synthesizing a TiO<sub>2</sub>-modified boron-doped diamond photoanode (BDD/TiO<sub>2</sub>) via electrophoretic deposition, detailing the chemical and electrochemical treatments applied to the bare BDD electrode prior to use. We provide a step-by-step guide for performing photoelectrochemical characterization under both dark and light conditions and describe an optical technique for investigating band-gap energy. For complete details on the use and execution of this protocol, please refer to Quilumbaquin et al.<sup>1</sup>.

  1. 2024 - Photoelectrocatalytic degradation of high-density polyethylene microplastics on TiO2-modified boron-doped diamond photoanode [Crossref]
  2. 2024 - Novel trends in mixed oxide electrodes for photoelectrocatalytic wastewater treatment
  3. 2019 - Overview of Thin Film Deposition Techniques [Crossref]
  4. 2023 - Structure, materials, and preparation of photoelectrodes
  5. 2016 - Charge Separation in TiO2/BDD Heterojunction Thin Film for Enhanced Photoelectrochemical Performance [Crossref]
  6. 2022 - Boron-Doped Diamond Electrodes: Fundamentals for Electrochemical Applications [Crossref]
  7. 2022 - Photoelectrocatalytic degradation of diclofenac with a boron-doped diamond electrode modified with titanium dioxide as a photoanode [Crossref]
  8. 2018 - Improvement of the degradation of Methyl Orange Using a TiO2/BDD composite electrode to promote electrochemical and photoelectro-oxidation processes [Crossref]
  9. 1998 - Diffuse Reflectance Spectrocopy