Design of a diamond-based in-vessel soft x-ray detector for the SPARC tokamak

MetadataDetails
Publication Date2024-09-01
JournalReview of Scientific Instruments
AuthorsStanley J. Normile, D. VĆ©zinet, C. Perks, F. Bombarda, G. Verona‐Rinati
InstitutionsUniversity of Rome Tor Vergata, Plasma Technology (United States)
Citations3

The in-vessel silicon diode arrays that are used for soft x-ray detection in many tokamaks are sensitive to neutron damage, making them unsuitable for burning plasma devices such as SPARC. In such a device, the silicon diodes would need to be placed far from the plasma—limiting their field of view—or an alternative detector could be used. Here, we present the design of a camera containing an array of chemical vapor deposition single-crystal diamonds, which will be placed in the upper and lower port plugs of the SPARC tokamak with a large enough view of the poloidal cross section to enable tomographic inversion. The camera design presented here is optimized to provide a wide field of view of the poloidal cross section. Simulated plasma conditions are used to estimate the x-ray signal that this detector array will receive and to fine-tune the camera placement within the tokamak.

  1. 2022 - Driven Rotation, Self-Generated Flow, and Momentum Transport in Tokamak Plasmas
  2. 2008 - Chapter 7: Tomography diagnostics: Bolometry and soft-x-ray detection [Crossref]
  3. 1988 - X-ray tomography on JET [Crossref]
  4. 1997 - Radiation-hardened x-ray imaging for burning-plasma tokamaks [Crossref]
  5. 1995 - D-T radiation effects on TFTR diagnostics (invited) [Crossref]
  6. 2021 - CVD diamond detectors for fast VUV and SX-ray diagnostics on FTU [Crossref]
  7. 2008 - Radiation tolerance of a high quality synthetic single crystal chemical vapor deposition diamond detector irradiated by 14.8Ā MeV neutrons [Crossref]
  8. 2010 - Single crystal artificial diamond detectors for VUV and soft x-rays measurements on JET thermonuclear fusion plasma [Crossref]
  9. 2023 - SPARC as a platform to advance tokamak science [Crossref]
  10. 1999 - Effects of neutrons on semiconductor x-ray detectors including n-type Joint European Torus and p-type GAMMA 10 tomography detectors [Crossref]