Experimental Verification of Inter Relation between Fowler–Nordheim and Millikan–Lauritsen Plot in Chemically Synthesized Zinc Oxide System

MetadataDetails
Publication Date2024-10-01
JournalMacromolecular Symposia
AuthorsPankaj Kumar, D. Banerjee
InstitutionsTeerthanker Mahaveer University

Abstract Cold cathode emission or cold field emission (CFE) is a purely quantum mechanical phenomenon and a phenomenon of wonder. The exact science behind the observed current ( I )-voltage ( V ) is yet to be pin pointed. For instance, a good cold emitter is very reasonably supposed to have low work function and good conductivity whereas a carbon allotropes like diamonds have just the reverse in both the cases, i.e., it is insulating in nature having very wide band gap as well as high work function yet it is considered to be an efficient field emitter. Since early of 20th century, till its middle a number of groups have suggested different equations or relations that can adequately describe the experimental CFE I - V characteristics adequately. Although they all fundamentally follow an exponential law, but so far, the relation suggests by Fowler and Nordheim (F-N) is the most accepted one. However, there is another relationship suggested by Millikan and Lauritsen (M-L) which is in spite of being reasonable not so common now a day to use. This work revisits different popular approaches for analyzing cold emission data. With this aim, the experimental CFE data obtained for chemically synthesized zinc oxide nanorods are chosen. The proper phase formation of ZnO is confirmed by XRD study whereas FESEM shows the rod like morphology. EDX confirms the proper stoichiometric ratio for the sample. After detail analysis it is confirmed that the theoretically proposed relation between F-N and M-L experimentally holds good as well and thus it would not be wrong to analyze the CFE data by simple M-L theory.

  1. 2017 - Field Emission Electronics [Crossref]