Effect of Magnetic Field on Thermal Conductivity of Nitrogen-Doped Diamond

MetadataDetails
Publication Date2025-01-01
JournalДоклады Российской академии наук Физика технические науки / Doklady Physics
AuthorsV.G. Ralchenko

The measurement of the thermal conductivity κ(T) of a single crystal of nitrogen-doped diamond in the temperature range from 6 to 92 K in a magnetic field of 14 T is reported. A weak effect of the magnetic field on κ(T) at low temperatures is found. The process of phonon scattering on bound charge carriers of an impurity under conditions of strong Zeeman splitting is discussed.