Quantum Technologies With Semiconductor Color Centers in Integrated Photonics
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2025-01-01 |
| Authors | Jelena VuÄkoviÄ |
Abstract
Section titled âAbstractâOptically interfaced spin qubits based on diamond and silicon carbide color centers are considered promising candidates for scalable quantum networks and sensors. However, they can also be used to build chip-scale quantum many body systems with tunable all to all interactions between qubits enabled by photonics - useful for quantum simulation and possibly computing. Full-text article not available; see video presentation