Surface Integrity of Silicon Carbide Machined by Diamond Wire Sawing - Effect of Feed Rate
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2025-01-01 |
| Authors | Natalie Souza Heinz, Lucas Cominetti Marchi, Gabriel Kons Cardoso, Fernando Moreira Bordin, Fabio Antonio Xavier |
Abstract
Section titled āAbstractāThis study investigates the influence of feed rate on the surface integrity of silicon carbide (SiC) machined by the diamond wire sawing (DWS) process. SiC is a ceramic material extensively used in st