Atomistic Simulation Study of Diamond Doping Based on Machine Learning Potential
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2025-01-01 |
| Journal | Physical Chemistry Chemical Physics |
| Authors | Yiheng Yan, Yaochen Yu, Junwei Hu, Xue-Cheng Sun, Qinlan Luo |
Abstract
Section titled āAbstractāDiamond is regarded as a highly promising semiconductor material due to its outstanding physical properties. However, achieving efficient p-type and n-type doping remains a significant challenge. In this work, weā¦