Boron-doped-diamond coupling with gold nanoparticles to prepare a simple and highly rigid aptasensor for detection of bleomycin

MetadataDetails
Publication Date2025-07-19
JournalBioelectrochemistry
AuthorsYilin Liu, Lei Wan, Danhong Zhang, Yibo Ma, Desheng Hu
InstitutionsJilin University, State Key Laboratory of Superhard Materials
Citations1

The innovative aptasensor consisting of β-mercaptohexanol (MCH), Aptamers, Au-NPs, and BDD (MAA-BDD) for the electrochemical detection of trace BLM is of excellent sensitivity, specificity, rigidity, and repeatability, which is suitable for further practical applications on trace BLM detection in various environments.

  1. 1971 - 3rd, Clinical study with bleomycin [Crossref]
  2. 2014 - DNA methylation reduces binding and cleavage by bleomycin [Crossref]
  3. 2021 - The experience of Intralesional bleomycin for orbital vascular anomalies
  4. 2023 - The efficacy of bleomycin sclerotherapy in the treatment of lymphatic malformations: a review and meta-analysis
  5. 2022 - Successful sclerotherapy for Cervicofacial macrocystic lymphatic malformations using Polidocanol and Pingyangmycin combined foam Sclerosants
  6. 2023 - Whole genome-based genetic insights of Bla(NDM) producing clinical E. Coli isolates in hospital settings of Pakistan
  7. 2024 - Allium cepa tests: exploring bleomycin induced cyto-genotoxicity and altered cell cycle kinetics in root tips meristematic cells [Crossref]
  8. 2021 - Butyrate improves skin/lung fibrosis and intestinal Dysbiosis in bleomycin-induced mouse models
  9. 2006 - Bleomycin and the skin [Crossref]