Abstract
Section titled âAbstractâIn the present study, the electronic structure and optical properties of P-2B co-doped diamond have been analyzed using first-principles calculations based on HSE06 generalized functions. Of the 15 complexes that we considered, the five most stable structuresâBCPCB system, PCCBCB system, PCBCCB system, PCBBCB system, and PBCB system were identified and studied, and the bandgap was found to reduce from 5.496 eV of intrinsic diamond to 3.610, 3.210, 3.210, 3.210, and 3.250 eV, respectively. Notably, the BCPCB-doped system exhibited significant changes in optical properties: the static dielectric constant increased from 4.18 to over 45, the real part of the conductivity showed a new peak at 2.0 eV (11) with a red-shifted spectrum, the light absorption edge was red-shifted, the static refractive index rose from 2 to 25, and a pronounced peak at 2.5 eV (16) was observed. These theoretical studies aim to support experimental research on P-2B doping in diamond to achieve p-type conductivity and enhanced optical properties.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2024 - (Invited) Preparation of N-Type and P-Type Doped Single Crystal Diamonds with Laser-Induced Doping and Microwave Plasma Chemical Vapor Deposition [Crossref]
- 2022 - Progress in semiconductor diamond photodetectors and MEMS sensors [Crossref]
- 2020 - Diamond semiconductor performances in power electronics applications [Crossref]
- 2020 - Comprehensive Analysis of Metal Modulated Epitaxial GaN [Crossref]
- 2016 - III-Nitride Double-Heterojunction Solar Cells With High In-Content InGaN Absorbing Layers: Comparison of Large-Area and Small-Area Devices [Crossref]
- 2001 - GaN and InGaN Metal-Semiconductor-Metal Photodetectors with Different Schottky Contact Metals [Crossref]
- 2022 - Recent progress in diamond radiation detectors [Crossref]
- 2021 - Surface transfer doping of diamond: A review [Crossref]
- 2011 - Thick boron doped diamond single crystals for high power electronics [Crossref]
- 2022 - Highly phosphorus-doped polycrystalline diamond growth and properties [Crossref]