Formation of low-resistance layer in diamond by ultraheavy N+ doping by ion implantation beyond the CVD doping limit
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Journal of Applied Physics |
| Published | 2026-02-18 |
| Authors | Kaiya Imamura, Yuhei Seki, Sakura Uehara, Junichi H. Kaneko, Yasushi Hoshino |
| DOI | 10.1063/5.0315014 |
Hot nitrogen ion implantation produced a diamond layer with (1.0 \times 10^{22}\ \mathrm{cm}^{-3}) nitrogen and room-temperature resistivity of about (100\ \Omega,\mathrm{cm}). The layer retained diamond crystallinity after implantation at 800 °C and annealing at 1300 °C. Its resistivity was comparable to the roughly (50\ \Omega,\mathrm{cm}) reported for phosphorus-doped CVD diamond near (1 \times 10^{20}\ \mathrm{cm}^{-3}). Hall measurements could not confirm carrier type because hopping conduction dominated.
Ion implantation and annealing
Section titled “Ion implantation and annealing”The experiments used optical-grade Type-IIa single-crystal diamond with a (001) surface and a (3 \times 3\ \mathrm{mm}^2) footprint. The material was synthesized by CVD, purchased, and polished to an atomic level. Chemical cleaning used an H2SO4 and HNO3 mixture at 300 °C for 30 minutes. A second NH3 and H2O2 mixture was applied at 80 °C for 20 minutes.
Nitrogen ions entered almost normal to the surface. Eight energies from 5 to 200 keV created a graded concentration profile. Each dose was selected in TRIM within SRIM2013 to make the profile uniform. SIMS measurements showed close agreement with the calculated profile. The authors attributed the small difference in the distribution tail to ion channeling.
Implantation ran at 800 °C on four substrates. The samples targeted (1.5 \times 10^{21}), (5.0 \times 10^{21}), (1.0 \times 10^{22}), and (3.5 \times 10^{22}\ \mathrm{cm}^{-3}). The (1.0 \times 10^{22}\ \mathrm{cm}^{-3}) sample required about 20 hours of implantation.
After implantation, the authors deposited an approximately 100 nm SiO2 cap by RF sputtering. The cap was intended to protect the surface during annealing at 1300 °C for 2 hours in Ar. A 5% HF etch removed the cap, followed by the chemical cleaning sequence. Prior RBS work found no silicon after these treatments, but clear oxygen. They therefore identified the final surface as oxygen-terminated.
Structural response to heavy doping
Section titled “Structural response to heavy doping”Raman measurements used a 532 nm laser and focused on the 1332 cm^-1 diamond peak. The signal sampled a depth of several hundred nanometers. A broad feature near 1430 cm^-1 came from nitrogen-vacancy center luminescence.
After implantation and annealing, the 1332 cm^-1 peak intensity fell by less than half. Its full width at half maximum changed little. No graphite-related Raman peaks appeared in samples up to (1.0 \times 10^{22}\ \mathrm{cm}^{-3}). The authors concluded that the implanted layer retained diamond crystallinity. The (1.0 \times 10^{22}\ \mathrm{cm}^{-3}) sample contained about 6 at. % nitrogen and remained optically transparent, with slight brown coloration.
At (3.5 \times 10^{22}\ \mathrm{cm}^{-3}), about 20 at. %, the doped layer instead transformed into graphite during annealing. Chemical cleaning then removed that layer.
RBS used a 1 MeV proton beam along the [001] direction and in a random geometry. Backscattered protons were detected at 110°. The (1.5 \times 10^{21}) and (5.0 \times 10^{21}\ \mathrm{cm}^{-3}) samples retained some crystallinity. Disorder increased with nitrogen concentration, consistent with the Raman results. Substitutional nitrogen can distort the lattice and raise the aligned yield. The authors warned that backscattering yield alone therefore cannot establish crystallinity.
Electrical transport and the role of nitrogen
Section titled “Electrical transport and the role of nitrogen”Four contacts each used Ti, Pt, and Au layers and were deposited at 600 °C. Each contact had a 500 µm diameter and sat near a corner of the substrate. Van der Pauw measurements covered eight adjacent-electrode combinations with polarity reversals, and the results were averaged. Hall measurements applied a constant 0.35 T field perpendicular to the sample. Constant current flowed between opposite electrodes, and Hall voltage was measured with both field polarities.
Room-temperature resistivity was about (1000\ \Omega,\mathrm{cm}) at (5.0 \times 10^{21}\ \mathrm{cm}^{-3}). It fell to about (100\ \Omega,\mathrm{cm}) at (1.0 \times 10^{22}\ \mathrm{cm}^{-3}). The resistivity plot against (T^{-1/4}) was more linear than the plot against (T^{-1}). The authors concluded that variable-range hopping dominated transport. They related lower resistivity to shorter hopping distances and stronger wave-function overlap.
The conventional donor model does not explain these values. Nitrogen’s donor ionization energy is about 1.4 to 1.7 eV. The authors used (N_D = 1.0 \times 10^{18}\ \mathrm{cm}^{-3}) and 0.01% compensation for a conventional activation estimate. The estimated room-temperature carrier concentration was below (1 \times 10^{-1}\ \mathrm{cm}^{-3}). Even assuming (1000\ \mathrm{cm}^2,\mathrm{V}^{-1},\mathrm{s}^{-1}) mobility, the calculated resistivity exceeded (10^{15}\ \Omega,\mathrm{cm}).
The (1.0 \times 10^{22}\ \mathrm{cm}^{-3}) sample gave linear room-temperature current-voltage curves for every electrode combination. The authors interpreted this behavior as ohmic contact. A carbon-implanted control at (1.5 \times 10^{21}\ \mathrm{cm}^{-3}) had higher resistivity than nitrogen-implanted diamond. Since carbon is not an effective donor or acceptor, the comparison suggests nitrogen caused the lower resistivity. The authors attributed the lower resistivity mainly to introduced nitrogen rather than implantation-induced defects.
Comparison with CVD and prior implantation
Section titled “Comparison with CVD and prior implantation”Hot implantation reached nitrogen concentrations far beyond the reported CVD limit. The highest cited CVD nitrogen concentration was (3.3 \times 10^{20}\ \mathrm{cm}^{-3}), obtained with NH3. Nitrogen implantation reached (1.0 \times 10^{22}\ \mathrm{cm}^{-3}) while retaining crystallinity.
| Doping route | Dopant concentration | Resistivity near room temperature | Reported outcome |
|---|---|---|---|
| Hot N implantation | (1.0 \times 10^{22}\ \mathrm{cm}^{-3}) | About (100\ \Omega,\mathrm{cm}) | Diamond crystallinity retained |
| CVD nitrogen | (3.3 \times 10^{20}\ \mathrm{cm}^{-3}) | Not stated | Highest concentration reported for CVD nitrogen |
| CVD phosphorus | About (1 \times 10^{20}\ \mathrm{cm}^{-3}) | About (50\ \Omega,\mathrm{cm}) | Partially usable n-type diamond |
Phosphorus remains the only donor incorporated through CVD that produced partially usable n-type characteristics, mainly on (111) surfaces. Its ionization energy is about 0.6 eV. The implanted nitrogen layer had a higher resistivity than the cited phosphorus value. The authors described the implanted layer as comparable to CVD-grown phosphorus-doped layers.
The same group previously reported hot boron implantation above (1 \times 10^{21}\ \mathrm{cm}^{-3}). That work achieved about (10^{-3}\ \Omega,\mathrm{cm}) with p-type conduction from room temperature to 800 °C. Phosphorus implantation had not achieved electrical activation, which the authors related to its larger atomic radius and high formation enthalpy.
Limits of the measured result
Section titled “Limits of the measured result”Hall data were unstable and insufficient to identify n-type behavior conclusively. The paper reports that n-type predominated in the measurements, but the authors did not derive a reliable carrier concentration. The low-resistance layer is therefore a hopping conductor with an unconfirmed carrier type, rather than a calibrated activated n-type region.
The strong nitrogen-vacancy luminescence suggested substitutional nitrogen. Some implanted nitrogen was probably paired with vacancies. Nitrogen-vacancy centers have an ionization energy around 2.8 eV, which the authors linked to the layer’s relatively high resistivity.
The highest tested dose also defined a structural boundary. Nitrogen at (3.5 \times 10^{22}\ \mathrm{cm}^{-3}) graphitized during annealing, while (1.0 \times 10^{22}\ \mathrm{cm}^{-3}) did not. The paper does not report implantation yield, sample-to-sample repeatability, or a reliable carrier mobility. A device process would also need to accommodate a 1300 °C anneal and an implantation lasting about 20 hours at the highest reported concentration.
Device implications
Section titled “Device implications”The authors propose hot nitrogen implantation for localized high-concentration n-type regions in diamond devices. Multiple ion energies provided depth-profile control, and SIMS agreed with the TRIM calculation. This creates a route beyond the CVD concentration limit without forming a graphite layer at (1.0 \times 10^{22}\ \mathrm{cm}^{-3}).
Linear current-voltage curves also support Ti/Pt/Au contacts on the (1.0 \times 10^{22}\ \mathrm{cm}^{-3}) layer. Device engineers should treat the region as a hopping-conductive implant until Hall measurements establish carrier density and stable type. The paper links this method to high-power, high-frequency, and energy-efficient diamond devices, but it does not demonstrate a complete device or a conventional activated channel.
Materials and support
Section titled “Materials and support”The study needs a (001) single-crystal diamond substrate and a Ti/Pt/Au contact stack for localized conductive regions in diamond electronic devices. The diamond materials catalog from 6CCVD lists MPCVD-grown single-crystal diamond plates and wafers with metallization options including Ti, Pt, and Au. The linked engineering support can be consulted for custom fabrication requirements for that implanted and annealed structure, while nitrogen implantation remains a separate process step.
View Original Abstract
We report the successful realization of low-resistance layer by high-concentration nitrogen doping in single-crystal diamond using high-temperature ion implantation. While nitrogen has been considered a potential donor in diamond, its deep donor level (∼1.7 eV) and difficulty of activation have limited its practical use in electronic applications. Furthermore, traditional CVD-based doping methods have been constrained by low solubility and poor depth control, with maximum reported N concentrations below ∼3×1020cm−3. In contrast, our approach enables the introduction of nitrogen at concentrations exceeding 1022cm−3 while suppressing the graphitization of the heavily doped region. Electrical measurements using the van der Pauw method revealed a strong dependence of resistivity on doping concentration, with room-temperature resistivity decreasing to ∼100Ωcm at a doping concentration of 1×1022cm−3. The achieved resistivity is comparable to that of phosphorus-doped diamond via chemical vapor deposition. Although precise carrier type and concentration could not be determined due to the dominance of hopping conduction, this study demonstrates, for the first time, that low-resistivity N-doped diamond layers can be fabricated via ion implantation. These results suggest that high-temperature ion implantation offers a practical pathway for forming localized and high-concentration n-type regions in diamond.
Boron Doped Diamond Electrode On Silicon
View Specs →
Electronic Grade Intrinsic Diamond Epitaxial Wafer H Terminated Superior 100 Mosfet Ready Substrate
View Specs →
Boron Doped Single Crystal Diamond Plate
View Specs →References we cover
Section titled “References we cover”- Ultraheavy boron doping of diamond by ion implantation for low-resistance layer formation - Effect of hot implantation
- Experimental Insights into Impurity Incorporation in Chemical Vapor Deposition Doped Diamond
- Diamond FinFET without Hydrogen Termination
- Inversion channel diamond metal-oxide-semiconductor field-effect transistor with normally off characteristics
Original source
Section titled “Original source”References
Section titled “References”- 2003 - Thin-film Diamond I: Semiconductors and Semimetals
- 2018 - Recent advances in diamond power semiconductor devices [Crossref]
- 1999 - A large range of boron doping with low compensation ratio for homoepitaxial diamond films [Crossref]
- 1999 - Growth and characterization of phosphorus doped n-type diamond thin films [Crossref]
- 2001 - Conductivity in boron-doped diamond [Crossref]
- 2005 - n-type doping of (001)-oriented single-crystalline diamond by phosphorus [Crossref]
- 2006 - Hall electron mobility in diamond [Crossref]
- 2007 - Carrier compensation in (001) n-type diamond by phosphorus doping [Crossref]
- 2010 - Hall hole mobility in boron-doped homoepitaxial diamond [Crossref]