Functionalizing Conductive Diamond - Recent Advance in Fabrication, Modifications, and Applications
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Carbon Energy |
| Published | 2026-02-16 |
| Authors | Ning Linghu, X. Jiang, Jing Xu |
| DOI | 10.1002/cey2.70169 |
| Citations | 1 |
Reviewed studies show that boron-doped diamond can serve as a durable electrode, catalyst support, sensor, and energy-storage interface. The material preserves a broad electrochemical window and low background current when sp³ content is high. One diamond-based supercapacitor retained 99.6% of its capacitance after 10,000 cycles, compared with about 85.2% for graphite and 75% for CNTs under similar conditions. The review explains conductive-diamond performance through growth chemistry, doping, termination, orientation, stress, and nanostructure. The authors compile published evidence from roughly the past decade. They do not report a new material or a unified experimental dataset.
Growth routes and process control
Section titled “Growth routes and process control”HPHT operates at 5 to 6 GPa and 1300°C to 1600°C with Co, Ni, or Fe catalysts. It grows bulk crystals, but pure hexagonal diamond remains difficult to obtain. CVD grows diamond from hydrocarbon and hydrogen gases at much lower pressure. Atomic hydrogen preferentially etches sp² carbon while stabilizing sp³ nuclei.
The review’s method summary gives the following deposition rates and tradeoffs.
| CVD process | Deposition rate | Area and review assessment |
|---|---|---|
| HFCVD | 0.1 to 3 μm h⁻¹ | Large area; lower quality; low cost |
| MWCVD | 0.2 to 20 μm h⁻¹ | 4 to 6 inch area; controllable quality; relatively high cost |
| DC arc plasma jet CVD | 10 to 25 μm h⁻¹ | 2 to 4 inch area; high growth rate; single-crystal use; high cost |
HFCVD uses CH4 or C2H2 in hydrogen with 2000°C to 2600°C filaments. Substrate temperatures of 700°C to 1000°C and pressures of 3 to 10 Torr promote dense nanocrystalline films. Methane above 6 vol% favors nanocrystalline diamond, while lower methane favors faceted microcrystals. Filament spacing, reactor geometry, and substrate cooling determine deposition uniformity.
MWCVD activates CH4/H2 with 2.45 GHz or 915 MHz microwaves at 700°C to 1000°C. Its filament-free design reduces metal contamination, but plasma edge effects and substrate temperature variation remain. DC arc plasma jet CVD produced 8-inch freestanding plates under dual magnetic fields. Three-point bending measured fracture toughness of 6 to 10 MPa m^(1/2). Reported fracture strengths were 580 to 1000 MPa. Other plates exceeded 1700 W m⁻¹ K⁻¹ in thermal conductivity.
Doping and termination control
Section titled “Doping and termination control”Boron introduces an acceptor level 0.37 eV above the valence-band maximum, producing p-type conductivity. Phosphorus and nitrogen introduce donor levels around 0.60 eV below the conduction-band minimum. Gas-phase incorporation controls doping directly but is limited by solubility and strain. Ion implantation adds spatial control but risks lattice damage. Multilayer doping can alter toughness by alternating doped and undoped layers.
Nanostructured BDD nanorod forests delivered 2820 μF cm⁻², about four orders of magnitude above planar BDD. Porous BDD made with nanoplatelet templates produced about 428-fold higher specific capacitance and remained stable over 12,000 cycles.
Hydrogen termination produced surface conductivity of 10⁻⁶ to 10⁻⁴ A V⁻¹. Carrier mobilities reached 365 cm² V⁻¹ s⁻¹. Removing C-H bonds lowered conductivity below 10⁻¹⁰ A V⁻¹. Hydrogen termination gives negative electron affinity. Oxygen termination gives positive electron affinity and reduced conductivity. Surface termination also changes wettability and electrochemical stability. Plasma, UV/ozone, anodic polarization, NH3 plasma, and silanization enable hydrogen, oxygen, and amine terminations.
Orientation, stress, and composite design
Section titled “Orientation, stress, and composite design”Crystal orientation changes dopant incorporation, oxidation, wear, and fracture. Boron is incorporated preferentially on (111) facets. Oxidation proceeds fastest on (110), followed by (100) and (111). Residual stress combines thermal mismatch during cooling from about 1150 K with distortion from defects and impurities. Raman spectroscopy tracks stress through shifts of the 1332 cm⁻¹ peak. X-ray diffraction with the sin² ψ method gives area-averaged stress. The curvature method uses Stoney’s formula during deposition.
Low-mismatch W and Mo substrates, porous structures, laser texturing, interlayers, controlled cooling, and annealing near 873 K can relieve stress. Annealing may generate graphite. Pure sp³ diamond is insulating, while moderate sp² content raises conductivity and capacitance. Excess sp² causes uneven transport and narrows the potential window. Diamond-graphene films reached 6.97 W m⁻¹ K⁻¹, twice the reported value for silicone pads.
Storage and cycle life
Section titled “Storage and cycle life”Porous BDD symmetric aqueous supercapacitors operated at 2.6 V. BDD micro-pyramids gave 53.7 mF cm⁻² at 2.54 mA cm⁻² and retained 95.5% after 5,000 cycles. CoNiO2/Co3O4 nanosheets on BDD reached 214 mF cm⁻² at 1 mA cm⁻². They retained 91.8% after 5,000 cycles.
An ultrastrong double-layer nanodiamond coating above 200 GPa blocked dendrite propagation. It produced Coulombic efficiency above 99.4% in full lithium-sulfur cells. Porous BDD with oxygen-vacancy MnO/C reached 381.8 mAh g⁻¹. It retained 92.6% after 560 cycles. BDD also supports earth-abundant Ce³⁺/Ce⁴⁺ and Mn²⁺/Mn³⁺ redox couples in flow batteries.
Electrolysis, disinfection, and recovery
Section titled “Electrolysis, disinfection, and recovery”BDD anodes generate hydroxyl radicals, ozone, and other reactive oxygen species. These oxidants support nonselective mineralization of organics under mild conditions. In textile wastewater, BDD removed 93% color, 75% TOC, and 48% COD. Ti/RuO₂-IrO₂ removed 88%, 62%, and 41% under optimized conditions. Three-dimensional porous BDD increases active area and improves fluid transport.
Disinfection reached 8-log inactivation of Pseudomonas aeruginosa through simultaneous ozone and free chlorine production. Chloride-containing water can instead generate perchlorate at levels up to 830 times the regulatory limit. Ultra-nanocrystalline BDD reduced perchlorate formation while retaining bactericidal activity. It used 0.08 Ah L⁻¹ at 25 mA cm⁻² in real effluent.
Paired electrolysis recovered up to 90% lithium leaching from spent LiFePO4. Phosphorus recovery reached 92% within 3 h. BDD extracted about 1.0 mg cm⁻² uranium within 11 h at 10 mg L⁻¹ U(VI). Recovery remained near 98% over 30 extraction-elution cycles. Hydrogen peroxide electrosynthesis reached 41% Faradaic efficiency in carbonate electrolytes. Pulsed current in a zero-gap PEM electrolyzer raised H₂O₂ yield nearly 70% over constant current.
Sensing and electrocatalysis
Section titled “Sensing and electrocatalysis”Screen-printed BDD detected lornoxicam at 9 × 10⁻⁸ mol L⁻¹. Diamond nanosheets on printed carbon detected Haemophilus influenzae at 1 CFU mL⁻¹ by electrochemical impedance spectroscopy. Oxygen-terminated BDD tracked seawater salinity for 90 days. Piezoresistive gauge factors reached 284, nearly twice the reported silicon value.
CO₂ reduction on pristine BDD gave formic acid Faradaic efficiency above 96%. Long-term electrical-to-chemical conversion efficiency remained close to 45%. Reduced BDD reached 64% Faradaic efficiency for CO. Its production rate was nearly three times that of nonactivated BDD. Boron-nitrogen codoping, amine termination, Pd decoration, and MXene modification changed product selectivity. Electrolyte composition also shifted the balance between formic acid and CO. Pt/BDD showed no activity loss after 2,000 oxygen-hydrogen cycling cycles in H₃PO₄ at 170°C. BiVO₄/BDD reached 3.3 mA cm⁻² under AM 1.5 irradiation. It removed 63.5% of tetracycline within 9 min.
Engineering limits and selection
Section titled “Engineering limits and selection”The authors identify unresolved issues in scalable growth, stress, doping, and termination. Defect-free single-crystal growth at reasonable cost remains unresolved. Thermal and intrinsic stress still limit film thickness, adhesion, optical performance, and carrier mobility. High-conductivity n-type doping remains difficult. Many surface terminations lose stability during operation. HFCVD electricity accounts for 40% to 60% of production expense. A 1 m² BDD film about 10 μm thick and single-sided costs $2200 to $3000. Growth rate, area, film quality, and cost differ sharply among CVD methods. Device selection must therefore couple doping and termination with substrate choice, residual stress, and electrode geometry. Pristine conductive diamond has low surface area and capacitance. Nanostructuring raises active area, while redox-active coatings raise capacitance further. The 99.6% retention applies to one reviewed supercapacitor under its reported conditions. It does not establish the same lifetime for every BDD electrode. A defensible comparison records dopant, termination, orientation, sp² fraction, substrate, growth rate, and residual stress. These variables change potential window, charge transfer, selectivity, and cycle life. The authors suggest machine learning to predict temperature variation and optimize methane/hydrogen ratios. They present this as a future control strategy, not a validated process model.
Materials and support
Section titled “Materials and support”For electrochemical electrodes, sensors, and energy-storage interfaces, the paper needs boron-doped diamond with controlled conductivity, termination, and active area. 6CCVD offers MPCVD-grown single-crystal and polycrystalline diamond, including boron-doped diamond, as plates and wafers up to 125 mm. The diamond materials catalog covers metallization with Au, Pt, Pd, Ti, W, or Cu, while engineering support is available for custom fabrication requirements.
View Original Abstract
ABSTRACT Conductive diamond, especially boron‐doped diamond, has gained tremendous attention due to its high stability, broad potential window, low background current, good biocompatibility, and tunable surface properties. Over the past 5 to 10 years, significant progress has been made in the synthesis and modification of conductive diamond, positioning it as a promising functional material in various electrochemical applications. This review covers synthesis methods, such as high‐pressure high‐temperature and chemical vapor deposition, highlighting their role in controlling diamond growth, microstructure, and doping. Modification strategies, including boron, nitrogen, and phosphorus doping, as well as surface terminations, crystal orientation, stress engineering, and hybridization, are discussed in terms of enhancing their electrochemical properties and expanding applications. Conductive diamond shows promise in energy storage, electrocatalysis, electrosynthesis, environmental remediation, and biosensing, particularly in supercapacitors, water treatment, and electrical detectors, owing to its robustness and stability. The review also discusses future directions, focusing on AI‐driven process optimization, advanced modifications, and the development of multifunctional diamond composites. This review aims to highlight the potential of conductive diamond in next‐generation electrochemical and energy technologies.
Boron Doped Diamond On Titanium Bdd Electrode
View Specs →
Boron Doped Diamond Electrode On Niobium Bdd Nb Electrode
View Specs →Boron Doped Diamond Electrode On Silicon
View Specs →References we cover
Section titled “References we cover”- Homogeneous spin-dephasing time of NV− centre in millimetre-scale 12C-enriched high-pressure high-temperature diamond crystals
- Improvement of morphology and electrical properties of boron-doped diamond films via seeding with HPHT nanodiamonds synthesized from 9-borabicyclononane
- Multifunctional diamond‐based catalysts - Promising candidates for energy conversions in extreme environments-A mini‐review
- Fast, Efficient Tailoring Growth of Nanocrystalline Diamond Films by Fine-Tuning of Gas-Phase Composition Using Microwave Plasma Chemical Vapor Deposition
- Ultrastable halide perovskite CsPbBr3 photoanodes achieved with electrocatalytic glassy-carbon and boron-doped diamond sheets
Original source
Section titled “Original source”References
Section titled “References”- 2017 - Nanodiamonds: Advanced Material Analysis, Properties and Applications