Recent Advances in Diamond-Capped GaN HEMTs for RF Application
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Nanomaterials |
| Published | 2026-02-09 |
| Authors | Yuanmeng Xiang, Mei Wu, Haolun Sun, Shiming Li, Hongda Chen |
| DOI | 10.3390/nano16040224 |
The review reports an all-around diamond integration that reduced the gate-electrode temperature of a GaN HEMT by 98 ± 19 °C at 9.5 W/mm. That measured result came from 500 nm diamond covering the top and sidewalls of a device fabricated on SiC. Sidewall diamond connected the cap to the substrate, while gate resistance measurements quantified the temperature change.
This cooling matched a 2.2 µm top-only diamond cap in the cited study. Diamond can therefore remove heat through a short path, but the interface and process determine how much benefit reaches the channel.
Measured thermal and RF gains
Section titled “Measured thermal and RF gains”An MCD-capped GaN MIS-HEMT reduced its measured maximum device temperature by 100 K at 25 W/mm. The 700 °C growth process preserved an on/off ratio of 10^6, while Idss rose from 0.9 to 1.1 A/mm. Peak transconductance rose from 102 to 148 mS/mm.
A 2025 top-side diamond device lowered its measured channel temperature by 111 °C at 24 W/mm. The same device kept fT at 23 GHz. The review attributes an 8.3% fmax decrease to gate resistance increasing from 15 to 25 Ω.
Diamond growth controls film quality
Section titled “Diamond growth controls film quality”Electrostatic seeding was the main reviewed method for nucleating diamond on GaN because it improves density and uniformity. A polymer-assisted dip-seeding study produced dense coverage and reduced compressive stress to 0.09 GPa. A weak Raman G band near 1800 cm^-1 indicated suppressed sp2-bonded carbon. Scanning electron microscopy measured grain size, while Raman spectroscopy tracked phase-related bands.
Mixed microdiamond and nanodiamond seeds filled interfacial voids and protected GaN from later plasma exposure. Two-stage MPCVD growth separated a mild nucleation stage from more aggressive film growth. Nucleation used 600 W, 20 Torr, and 700 °C, followed by 1600 W and 70 Torr for main growth. The resulting films reached about 400 W/(m·K) at 600 nm and about 600 W/(m·K) at 900 nm. A cited integrated result reported a channel temperature reduction of up to 150 °C at 15 W/mm.
A three-step process lowered growth temperature to 400 °C by using oxygen to generate OH radicals. It produced 659 nm grains, 97.1% phase purity, and 300 W/(m·K) thermal conductivity. The first nucleation stage used 3.4% CH4 and produced a Raman sp3 peak FWHM of 6.6 cm^-1.
Interface engineering sets the thermal limit
Section titled “Interface engineering sets the thermal limit”A high interface TBR can dominate the thermal path despite diamond’s high bulk conductivity. GaN and diamond have thermal expansion coefficients of 5.2 × 10^-6 and 0.7 × 10^-6 K^-1, respectively. Protective SiNx, SiO2, or Al2O3 interlayers limit hydrogen plasma damage but add thermal resistance.
An in situ 20 nm SiNx layer produced TBR of 52.8 m²·K/GW. A later structure combined 1.5 µm PCD with 20 nm PECVD SiNx and measured 313.68 W/(m·K) effective diamond conductivity. Time-domain thermoreflectance gave 39.35 m²·K/GW for the diamond/GaN TBR. Simulation for that structure predicted a 17.1 °C device-temperature reduction at 15 W/mm.
Diamond deposition raised the measured tensile strain from 58.14 to 155.81 MPa and 2DEG density by 4.9%. Thinning SiNx from 10 nm to about 2 nm lowered TBR to 12.8 ± 0.64 m²·K/GW.
The lowest reviewed value was 3.1 ± 0.7 m²·K/GW with less than 1 nm SiNx remaining after growth. Controlled nucleation at 600 W and 20 Torr limited SiNx etching, while carbon diffusion formed a graded SiC transition region. A 10 nm ta-C interlayer gave 13 m²·K/GW, with 2 to 3 nm converted to UNCD during MPCVD.
A temperature sweep from 740 to 860 °C found minimum effective TBR of about 24 m²·K/GW at 800 °C. At 740 °C it was about 96, while at 860 °C it was about 60 m²·K/GW. Simulation at 800 °C predicted a 23% peak-temperature reduction, from 185 °C to 142.3 °C, for a 1.5 µm cap.
Patterned GaN grooves with 200 nm pitch and 320 nm depth lowered TBR from 51 to 25 m²·K/GW after 1 µm diamond growth.
Simulation exposes thermal and RF tradeoffs
Section titled “Simulation exposes thermal and RF tradeoffs”Three-dimensional simulations found 8.8% to 33.9% lower peak junction temperatures for 1 to 14 µm diamond caps. A package-level simulation replaced SiNx passivation with 500 W/(m·K) PCD at 6.0 W/mm. Maximum junction temperature fell from 105.8 °C to 98.2 °C, while temperature nonuniformity fell from 18% to 8%.
RF co-simulation showed that passivation thickness and dielectric constant affect fT and fmax. Without passivation, fT was 106 GHz and fmax was 270 GHz. Fifty nanometers of SiNx reduced them to 86 GHz and 225 GHz, while 2.7 µm BCB reduced them to 84 GHz and 217 GHz.
For a 0.6 to 2.7 µm diamond passivation, fT declined from 98 to 85 GHz. At 1.0 µm thickness, raising the relative dielectric constant from 2.3 to 4.0 lowered fT from 96 to 91 GHz. The same change lowered fmax from 243 to 227 GHz. The authors attributed this attenuation to the capacitance introduced by diamond passivation.
Thermal spreading and RF behavior therefore require simultaneous optimization of thickness and dielectric constant.
Etching and integration determine compatibility
Section titled “Etching and integration determine compatibility”Conventional diamond CVD requires 600 to 800 °C, while hydrogen-rich plasma can etch GaN and damage Ni/Au gates. Gate-last integration grows and patterns diamond before fabricating the gate, avoiding direct heat exposure of the finished gate. Gate-first integration grows diamond after gate fabrication and therefore needs heat-resistant metal or a metal-insulator-semiconductor gate. The review identifies gate-last as more common, but describes gate-first as favorable for large-area diamond deposition.
Two-step diamond etching first used high-power O2/Ar ICP to remove about 90%, then low-power O2 for the remaining 10%. The low-power etch ran at one-tenth the high-power rate and preserved the nanocrystalline grain structure. A cyclic Ar, O2, and SF6 process with cooling steps produced a diamond surface roughness below 1 nm RMS.
A multi-step process achieved 0.5 µm etching precision and fabricated a HEMT with a 0.5 µm gate. It produced Idss of 950.45 mA/mm at VGS = 1 V, 27.9% above a conventional AlGaN/GaN HEMT. Its fT reached 34.6 GHz, and its average gain at 10 GHz was 36.7% above the reference.
A combined dry and wet process removed a 20 nm SiNx hard mask with diluted HF after diamond etching. It produced a damage-free AlGaN/GaN surface, reduced self-heating by about 42.6%, and raised peak gm from 117.2 to 127.6 mS/mm. The off-state drain current remained 3.49 × 10^-4 mA/mm, nearly identical to the reference.
These results show that etch selectivity and surface damage can be as important as cap conductivity.
Limits and selection guidance
Section titled “Limits and selection guidance”Actual MPCVD PCD conductivity is typically several hundred to 1000 W/(m·K), well below the cited bulk value of about 2000 W/(m·K). Material selection should therefore use measured in-plane and cross-plane conductivity for the intended film thickness. Engineers should specify interface TBR alongside conductivity because reported effective and interface TBRs span 3.1 to 96 m²·K/GW.
Cap thickness also needs an RF penalty check, since 0.6 to 2.7 µm diamond passivation reduced simulated fT. Growth temperature must fit the gate stack and plasma exposure, rather than being selected only for film quality. Even low-temperature growth at 450 to 500 °C increased gate leakage 4.8 times, although annealing reduced it.
The paper identifies coupled thermal, electric, and stress models as future work. It also calls for dynamic thermal analysis and long-term models that include material degradation. An effective design records channel temperature, TBR, fT, fmax, and leakage together under the intended power condition. Measured cooling remains the main benefit, but interface resistance, RF attenuation, and process damage set the usable limit.
Materials and support
Section titled “Materials and support”The paper requires an MPCVD-grown polycrystalline diamond cap for near-junction heat spreading, with device examples using 150 nm to 1.5 µm films. 6CCVD’s diamond materials catalog includes MPCVD-grown polycrystalline diamond from 0.1 to 500 µm thick, polished below 5 nm Ra for inch-size material.
The linked engineering support can define the Au, Pt, Pd, Ti, W, or Cu metallization and custom fabrication requirements for the paper’s integration routes.
View Original Abstract
Self-heating effects severely limit the performance of gallium nitride high-electron-mobility transistors (GaN HEMTs) in high-power radio frequency (RF) applications. Diamond capping technology leveraging diamond’s exceptional thermal conductivity (>2000 W/m·K) has emerged as a highly promising near-junction cooling solution. However, its integration with GaN HEMTs faces challenges including lattice/thermal mismatch, high thermal boundary resistance (TBR), and process compatibility. This review summarizes recent progress in high-thermal-conductivity diamond film growth, TBR optimization, thermal simulations, and the integrated process with GaN devices. These technological breakthroughs enable diamond-capped GaN HEMTs with an excellent comprehensive performance. Continued advances in these fields will be critical for fully releasing the capabilities of diamond capping technology for GaN HEMTs in high-frequency and high-power applications.
Advanced Thermal Simulation Service Diamond Heat Spreader Performance Analysis
View Specs →
Free Standing Polycrystalline Cvd Diamond Membrane
View Specs →
Free Standing Boron Doped Diamond Pcd Film
View Specs →Original source
Section titled “Original source”References
Section titled “References”- 1993 - High electron mobility transistor based on a GaN-AlxGa1−xN heterojunction [Crossref]
- 2001 - Band parameters for III-V compound semiconductors and their alloys [Crossref]
- 2014 - A Survey of Wide Bandgap Power Semiconductor Devices [Crossref]
- 2018 - Emerging trends in wide band gap semiconductors (SiC and GaN) technology for power devices [Crossref]
- 1994 - Microwave performance of a 0.25 μm gate AlGaN/GaN heterostructure field effect transistor [Crossref]
- 2004 - 30-W/mm GaN HEMTs by field plate optimization [Crossref]
- 2019 - GaN-On-Diamond HEMT Technology With TAVG = 176 °C at PDC, max = 56 W/mm Measured by Transient Thermoreflectance Imaging [Crossref]