Nanophotonic waveguide chip-to-world beam scanning
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Nature |
| Published | 2026-03-11 |
| Authors | Matt Saha, Y. Henry Wen, Andrew S. Greenspon, Matthew Zimmermann, Kevin J. Palm |
| DOI | 10.1038/s41586-025-10038-6 |
| Citations | 2 |
A CMOS-fabricated photonic ski-jump reached a footprint-adjusted spot rate of 68.6 mega spots s⁻¹ mm⁻². The result exceeded the best micro-electro-mechanical system mirrors in the authors’ comparison by more than 50-fold. They state that this rate can support one million pixels at 100 Hz from an approximately 1.5 mm diameter footprint.
Performance and benchmarks
Section titled “Performance and benchmarks”The device couples a nanoscale Si₃N₄ waveguide to a piezoelectric cantilever that curls approximately 90° out of plane. Its active footprint is less than 0.1 mm², and the authors describe its submicrometre output as diffraction-limited.
The authors define the net figure of merit, called FOM, as footprint-adjusted spot count multiplied by refresh rate. Conventional pupil-plane scanners in their analysis produce approximately 500,000 to 1 million spots s⁻¹ mm⁻². Focal-plane scanners remain below 50,000 spots s⁻¹ mm⁻² because their bulk implementation lacks a scalable, actuated single-mode waveguide. The ski-jump FOM exceeds the paper’s fibre-scanner reference by more than 1,000-fold. It also exceeds the quoted MEMS mirrors and acousto-optic deflectors by more than 50-fold.
These comparisons use a simplified metric that does not include size, weight, power and cost. The 64 ski-jump array had a curvature distribution with a standard deviation below 2%. The authors project that compact tiling with a 10× FOM increase could support giga-spot light engines at 1 kHz within a sub-5-cm chip area. This gigaspot performance is a projection, not a measured array result.
Device construction and actuation
Section titled “Device construction and actuation”Fabrication used a 200 mm volume CMOS process joining Si₃N₄ photonics with AlN piezoelectric actuators. The cantilever is about 2 µm thick and has submicrogram mass. The lower and upper layer sets are each about 1 µm thick. The sequence contains SiO₂, Al, AlN, Al, SiO₂, Si₃N₄ and final SiO₂.
Fabrication deposited amorphous silicon beneath the device layers and patterned release holes every 30 µm. XeF₂ etching removed the amorphous silicon after wafer fabrication, leaving the cantilever clamped at one end. Cross-ribs in the upper SiO₂ controlled lateral and longitudinal curvature, producing the passive out-of-plane curl.
The standard Si₃N₄ waveguides were 400 nm wide and 300 nm thick. They tapered to 200 nm at the tip for the reported devices. Applying voltage across aluminium electrodes generated piezoelectric stress in AlN and deflected the cantilever. White-light profilometry measured a longitudinal displacement of about 29.4 µm during direct-current actuation from minus 50 V to plus 50 V. The reported direct-current hold power was approximately 10 nW at 20 V.
Beam quality and mechanical response
Section titled “Beam quality and mechanical response”The waveguide was designed for single-mode propagation near 737 nm, the zero-phonon line of silicon vacancy colour centres in diamond. At the tapered tip, the measured mode field diameter was 0.66 µm along x and 0.50 µm along y. The corresponding fundamental mode half-angle divergences were 41° and 53°. An on-resonance test with a supercontinuum source demonstrated transmission from 450 nm to 750 nm.
The mechanical modes included longitudinal Y motion and lateral X motion, with frequencies set by stress, stiffness and geometry. The Y1 mode swept nearly circular arcs, while Y2 and X1 produced nearly flat tip trajectories. Stroboscopic ICCD imaging recorded these trajectories. Finite-element simulations agreed with the characteristic modes of a passively curled, singly clamped cantilever.
Reducing pressure raised the resonant response by as much as 30 dB. Ambient measurements gave a quality factor near 5, while high vacuum below 0.1 mTorr raised the fundamental longitudinal Q to approximately 10,020. At high vacuum, ambient-level displacement required approximately one hundredth of the ambient drive voltage. Rough vacuum at 1.15 Torr gave intermediate quality factors, and measurements also covered cryogenic operation at 6.9 K. A PID control loop located and tracked the resonance, with the scan range stable after reaching steady state.
Two-dimensional scanning
Section titled “Two-dimensional scanning”Each cantilever base carried bilateral aluminium electrodes that could apply independent X and Y drive signals. Different frequencies and relative phases excited orthogonal resonances, producing Lissajous trajectories. In one demonstration, 4.83 kHz and 6.44 kHz drives produced a 3:4 pattern with a 1.61 kHz refresh rate. A 37.2 kHz and 6.2 kHz pair produced a 6:1 pattern with a 6.2 kHz refresh rate. Out-of-phase electrode signals suppressed the Y response while increasing the X response. The authors selected the second-order Y mode and fundamental X mode because their combination produced a sufficiently flat scan area.
Off-chip current-controlled laser diodes supplied the optical modulation for full-colour images and video. A 1,450 µm long device in vacuum projected full-fill patterns at 1.561 kHz and 2.639 kHz, with a 7 Hz refresh rate. A 950 µm device in vacuum projected at 4.716 kHz and 6.408 kHz, with a 36 Hz refresh rate. High-fill and high-rate patterns remained stable during driving for more than 15 h. Direct-current operation showed no hysteresis, while one-dimensional resonant scanning remained stable for more than one billion cycles and dozens of hours.
Silicon vacancy control in diamond
Section titled “Silicon vacancy control in diamond”A fibre-packaged ski-jump was aimed at a diamond microchiplet containing eight waveguides with implanted, negatively charged silicon vacancies. The sample sat in a Montana 4 K cryostat, and light near the approximately 737 nm zero-phonon line was routed to each waveguide. The authors tuned to the C transition of one frequency-resolved emitter and aligned the static output with one channel. The measured second-order autocorrelation was g⁽²⁾(0) = 0.09 with an uncertainty of 0.09, below the stated 0.5 single-photon threshold.
Periodic initialization used a 6.34 kHz oscillation with the emitter at the apex of the device’s motion. The phonon sideband fluorescence gave a 27.5 dB extinction ratio and a 157 µs repetition time. The standard deviation of the integrated pulse area was 0.003. Scattered light limited the reported extinction ratio.
Ensemble excitation addressed six distinct diamond waveguides while the beam scanned across them. One damaged taper scattered most of the resonant excitation, showing that tip quality affects channel delivery. The authors propose that one ski-jump could control thousands of optical channels. That claim remains an architectural projection rather than a measured channel count. A proposed cryogenic architecture could keep the photonic control system on a warmer stage beside the quantum processor.
Scaling limits and diamond integration
Section titled “Scaling limits and diamond integration”Longer, thinner cantilevers and tapered or segmented widths can reduce air damping, according to the authors’ scaling analysis. An untapered waveguide cross-section reduced beam diameter by about 40%, increased spot density 2.8-fold and increased scan speed 1.7-fold. Longer ranges raise speed and area but reduce refresh rate, while multiple waveguides raise fill factor at the cost of more routing channels.
Optimal performance currently requires resonant operation in vacuum. Die-level vacuum packaging is needed for low-pressure operation without a bulky chamber. An iPhone 15 Pro lens produced a 1.69 µm Airy radius, close to the 1.67 µm Rayleigh limit for its f/1.78 design. Curved scan trajectories can defocus onto sensors designed for flat image planes. Optical and mechanical compensation can address this problem, but the paper does not demonstrate a complete packaged imager. Resonant scanning lacks true random access, although switching emission among devices can provide coarse pointing. Higher optical powers may cause waveguide nonlinearities or thermal loading, which established control and heat-management methods could mitigate.
For diamond integration, the demonstration makes alignment, spectral matching and taper quality practical requirements. The beam must overlap a silicon vacancy channel near 737 nm while retaining submicrometre spatial confinement. Repeated optical addressing requires stable phase and amplitude. The paper does not compare diamond crystals, vacancy concentrations or surface treatments, so it cannot specify the best diamond material.
View Original Abstract
A seamless chip-to-world photonic interface enables broad advancements in optical ranging, display, communication, computation and quantum information science. The ideal solution enables two-dimensional scanning of a diffraction-limited beam from anywhere on a photonic integrated circuit to a large number of resolvable spots. Current beam-scanning technologies are limited by a fundamental trade-off: photonic-integrated-circuits with diffractive optics offer scalability but have poor mode quality1,2, whereas inertially limited micromechanical scanners provide high-quality beams but lack scalable integration3,4. Here we report a photonic ski-jump—a nanoscale waveguide monolithically integrated on a piezoelectric cantilever—to overcome these limitations. It passively curls ~90° out-of-plane within a less-than-0.1 mm2 footprint, emits a submicrometre, broadband diffraction-limited beam, and exhibits kilohertz-rate mechanical resonances with quality factors of over 10,000. Fabricated in a volume complementary metal-oxide-semiconductor (CMOS) foundry, our device enables scalable two-dimensional beam scanning. Driven on-resonance at CMOS-level voltages, it achieves a footprint-adjusted spot rate of 68.6 mega spots s-1 mm-², exceeding state-of-the-art micro-electro-mechanical systems mirrors by more than 50-fold, which is sufficient for one million pixels at 100 Hz from an approximately 1.5 mm diameter footprint. We demonstrate full-colour image and video projection, and single-photon initialization and readout from silicon vacancy centres in diamond. Finally, by demonstrating uniformity across a 64 ski-jump array, we establish a pathway to achieving greater than one gigaspot resolution at kilohertz rates within a sub-5-cm-diameter footprint, creating a seamless optical pipeline between integrated photonic processors and the free-space world. A monolithically integrated photonic ski-jump enables scalable, diffraction-limited 2D beam scanning from photonic chips, achieving ultrahigh spot rates, compact footprints and applications spanning displays, sensing and quantum photonics.
Electronic Grade Intrinsic Diamond Epitaxial Wafer H Terminated Superior 100 Mosfet Ready Substrate
View Specs →
Diamond Epitaxial Wafer For Diodes 2
View Specs →