Multichannel highly sensitive diamond quantum magnetometer
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Journal of Applied Physics |
| Published | 2026-04-13 |
| Authors | A. Yoshimura, A. Kanamoto, Naota Sekiguchi, Chikara Shinei, Masashi Miyakawa |
| DOI | 10.1063/5.0303834 |
A single continuous-wave optically detected magnetic resonance module measured two points 3.6 mm apart. Its reported filtered sensitivities were 21 and 22 pT/√Hz over a 25 to 300 Hz bandwidth. Frequency-division multiplexing kept both readings simultaneous. Differencing the readings improved the gradiometric sensitivity to 14 pT/√Hz.
Frequency-division multiplexed readout
Section titled “Frequency-division multiplexed readout”Each NV-center ensemble was excited with a green laser, and one photodiode collected fluorescence from both ensembles. Different bias fields moved their magnetic resonances into separate frequency regions. The microwave drive used separate center frequencies and frequency-modulation frequencies for each point. The modulation frequencies were 7.5 kHz and 10 kHz. A field change at either point then appeared in the shared fluorescence trace at its assigned modulation frequency. Two lock-in amplifiers recovered the ODMR signals independently.
Separate PID regulators held the microwave center frequencies on their resonance frequencies. The PID bandwidth was 200 Hz. The lock-in low-pass filters had a 3 dB cutoff frequency of 1 kHz. Frequency shifts supplied by the PID loops represented the measured field changes through the NV-center gyromagnetic ratio. This arrangement produced simultaneous real-time measurements from one fluorescence collection path.
Diamond samples and NV-center preparation
Section titled “Diamond samples and NV-center preparation”The authors cut two sensing elements from one HPHT-grown diamond crystal. Both had (111) surface orientations, 1.2 × 0.8 mm² area, and 0.3 mm thickness. ESR gave an initial substitutional nitrogen concentration of 1.8 ppm. A 12C-enriched carbon source reduced the 13C concentration to about 50 ppm.
Electron irradiation used 2 MeV energy and a total fluence of 1 × 10¹⁸ cm⁻². The samples were then annealed at 1000 °C for 2 h under vacuum. ESR gave residual substitutional nitrogen and negatively charged NV-center concentrations of 0.3 and 0.2 ppm, respectively. An independent measurement gave a T2* of about 4.6 μs.
Each ensemble was excited at 532 nm. The laser spot had a 100 μm 1/e² diameter, and each beam had an intensity of about 1.1 W. Hemispherical lenses and a tube with an elliptical reflective inner surface collected fluorescence. A 650 nm long-pass filter rejected scattered laser light. Balanced detection reduced excitation-laser intensity noise.
Bias-field control and spectral separation
Section titled “Bias-field control and spectral separation”The bias field lay along the z axis of the (111) crystal orientation. A permanent magnet supplied a common field of about 1 mT. Series-connected coils modified the field in the same direction at diamond 1 and the opposite direction at diamond 2. Their geometry placed the two diamonds at extrema of the calculated field profile. This placement reduced field inhomogeneity within each excitation spot and the resulting ODMR peak broadening.
The calculated field profile used 25 mA. The measured field-to-current ratios were 0.60 ± 0.02 and −0.65 ± 0.02 μT/mA. At the operating bias, the field difference between diamonds was 42 μT. Each ODMR peak had a linewidth of about 200 kHz, well below the 2.16 MHz hyperfine splitting. Each ensemble therefore had an independently usable resonance within the same hyperfine manifold.
A 0.1 mm thick copper foil carried the microwave field to both diamonds. The drive included all three hyperfine transitions to improve ODMR contrast. A 2.16 MHz RF field mixed with the microwaves enabled that three-tone excitation.
Calibration and bandwidth
Section titled “Calibration and bandwidth”The two-point system was calibrated by applying a sinusoidal coil-current modulation at 30 Hz. The applied field amplitude was calculated from the independent coil calibration. The measured-to-applied slopes were 1.02 ± 0.01 for diamond 1 and 0.97 ± 0.01 for diamond 2. Their proximity to unity supports accurate recovery of the applied field amplitudes. The main uncertainty in the applied amplitude came from the coil calibration constants.
The response of diamond 1 was also measured over frequency. The response reached 3 dB below its low-frequency value at 300 Hz. The measured 3 dB bandwidth was therefore 300 Hz. This agreed approximately with the 200 Hz PID feedback bandwidth, which limited the measurement bandwidth.
Sensitivity and environmental noise
Section titled “Sensitivity and environmental noise”The authors measured the output noise without magnetic shielding. Both diamonds showed a noise-density floor of about 15 pT/√Hz at and above roughly 100 Hz. Noise below 25 Hz increased because of environmental fields. A nearby flux-gate sensor recorded similar low-frequency behavior, and trains about 20 m away were identified as an environmental source.
A flux-gate sensor with a 3.5 mm diameter, 22 mm long detection coil served as the environmental reference. Its noise floor was estimated at about 15 pT/√Hz from measurements inside a magnetic shielding box.
Noise peaks near 90 and 200 Hz had no identified source. The authors found that they decreased in the difference of the two outputs. They therefore treated these peaks as common-mode magnetic noise and suspected environmental variation. This interpretation remained a suspicion because the peaks were not traced to a specific source.
The sensitivity calculation used digital notch filters for the environmental peaks and a digital bandpass filter with 3 dB cutoffs at 25 and 300 Hz. The authors defined the sensitivity as the field detectable with a signal-to-noise ratio of 1 over the measurement time. The resulting sensitivities were 21 and 22 pT/√Hz for diamonds 1 and 2, respectively. These are filtered sensitivities in the stated band, rather than unfiltered broadband values.
The difference signal reached 14 pT/√Hz because common-mode environmental noise was reduced. Estimated photon shot-noise limits were 6.1 and 7.5 pT/√Hz. They were calculated from the detected fluorescence photocurrent and the zero-crossing slope of the ODMR peak. The measured sensitivities were above those limits, while the gradiometric result showed that common-mode environmental noise dominated much of the remaining excess.
Scaling limits and engineering implications
Section titled “Scaling limits and engineering implications”The experiment demonstrated two channels, although the authors propose expansion to more points. Its 3.6 mm spacing was selected for measuring the spatial distribution of brain magnetic fields in small animals such as rats. Earlier gradiometers had achieved real-time measurements at two points with millimeter-scale spacing, but scaling their point count while retaining close spacing remained difficult. Infrared-absorption DQMs had demonstrated either high sensitivity or real-time multipoint operation, but not both at once. At 3.6 mm, the present experiment retained simultaneous two-point readout with 21 and 22 pT/√Hz.
The present spacing was limited by the 100 μm excitation spot and the bias-field geometry. Overlapping laser spots would overlap the ODMR peaks in frequency and prevent independent readout. The authors suggest reducing the spot to the micrometer scale. They also propose acousto-optic deflectors or spatial light modulators for multipoint illumination. Micromagnets or microcoils could produce the required bias field at the submillimeter scale. These changes were proposed, not demonstrated.
Adding channels also requires enough spectral room and field homogeneity. The finite ODMR linewidth limits multiplexing within the hyperfine manifold. A larger bias-field difference could move peaks outside that manifold, but it generally worsens field homogeneity. The authors identify perfectly aligned NV centers as a way to reduce the number of ODMR peaks and leave more frequency space for multiplexing.
For device engineering, orientation, nitrogen concentration, spin coherence, laser geometry, and bias-field uniformity set design constraints. The demonstrated (111) samples supported a 42 μT resonance separation and a 100 μm readout spot. A denser array therefore requires coordinated changes to the diamond, excitation system, and local field control.
Materials and support
Section titled “Materials and support”The magnetometer needs two 0.3 mm thick single-crystal diamond plates with NV-center ensembles for two-point sensing. The reported samples were HPHT-grown with (111) surfaces. 6CCVD’s diamond materials catalog lists MPCVD-grown single-crystal plates from 0.1 to 500 micrometers thick, so the linked engineering support should review material equivalence and the optical and microwave access required for a custom assembly.
View Original Abstract
We demonstrate a highly sensitive real-time magnetometry method at two measurement points. This magnetometry method is based on the frequency-division multiplexing of continuous-wave optically detected magnetic resonance. We use two ensembles of nitrogen-vacancy (NV) centers separated by 3.6 mm to measure a magnetic field. A different bias field is applied to the two NV ensembles to resolve the resonance peak for each ensemble in the frequency space and enables the multiplexed magnetometry at the two points. The sensitivities achieved at the measurement points are 21 and 22pT/Hz. The proposed magnetometry method can be expanded to include more measurement points and shorter spacing. The capability of real-time measurement at numerous points with short spacing and high sensitivity is beneficial for various applications, including biomagnetic sensing, geophysical research, and material science.
High Concentration Quantum Grade Single Crystal Diamond
View Specs →Products
View Specs →
Single Crystal Cvd Diamond Plate
View Specs →References we cover
Section titled “References we cover”- Towards high-sensitivity magnetometry with nitrogen-vacancy centers in diamond using the singlet infrared absorption
- Diamond-on-chip magnetic field camera for mobile imaging
- Millimetre-scale magnetocardiography of living rats with thoracotomy
- Multiplexed Sensing of Magnetic Field and Temperature in Real Time Using a Nitrogen-Vacancy Ensemble in Diamond
- Diamond Magnetometry and Gradiometry Towards Subpicotesla dc Field Measurement
Original source
Section titled “Original source”References
Section titled “References”- 2024 - 2024 roadmap on magnetic microscopy techniques and their applications in materials science [Crossref]
- 2023 - Quantum sensors for biomedical applications [Crossref]
- 2020 - Sensitive magnetometry in challenging environments [Crossref]
- 2020 - Sensitivity optimization for NV-diamond magnetometry [Crossref]
- 1993 - Magnetoencephalography—theory, instrumentation, and applications to noninvasive studies of the working human brain [Crossref]
- 2016 - SQUIDs in biomagnetism: A roadmap towards improved healthcare [Crossref]
- 2022 - Millimetre-scale magnetocardiography of living rats with thoracotomy [Crossref]
- 2025 - Performance evaluation of a diamond quantum magnetometer for biomagnetic sensing: A phantom study [Crossref]
- 2016 - Optical magnetic detection of single-neuron action potentials using quantum defects in diamond [Crossref]