ПІДВИЩЕННЯ ЕФЕКТИВНОСТІ ВИКОРИСТАННЯ АЛМАЗНИХ ШЛІФУВАЛЬНИХ КРУГІВ НА ОРГАНІЧНОМУ ЗВ'ЯЗУЮЧОМУ МАТЕРІАЛІ ШЛЯХОМ РОЗРАХУНКУ РАЦІОНАЛЬНОЇ СТРУКТУРИ ТА ВИКОРИСТАННЯ УЛЬТРАДИСПЕРСНОГО АЛМАЗУ
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | The Scientific Issues of Ternopil Volodymyr Hnatiuk National Pedagogical University Series pedagogy |
| Published | 2026-05-15 |
| Authors | Євгеній Островерх |
Adding about 1 wt% detonation nanodiamond to an SFP-012A polymer binder raised Vickers microhardness from 78 HV to 96 HV, a 23% increase. The gain was measured on sintered 125 x 3 x 3 mm rings with a 50 g load and a 136° diamond pyramid. This result concerns binder hardness, not a direct increase in wheel life or grinding throughput.
Rationale for modifying the binder
Section titled “Rationale for modifying the binder”Organic binders account for more than 55% of produced binders because they are easy to manufacture and low in cost. The literature review reports that more than half of diamond loss comes from grains falling out of the binder. It also states that current binders allow the abrasive to use no more than 20% of its potential.
These figures make grain retention and binder strength design targets rather than secondary processing choices. For this study, binder hardness was the measured endpoint. Wheel life, grain pullout, and grinding temperature were not measured directly.
Specimen design and preparation
Section titled “Specimen design and preparation”SFP-012A is a bakelite binder based on the SF-012 phenol-formaldehyde oligomer and a hexamethylenetetramine curing agent. The control was B2-01 based on SFP-012A with 6 wt% hexamethylenetetramine. The modified series used SFP-012A, filler, 6 wt% GMTA, and 0.5, 1, or 2 wt% nanodiamond. B2-01 contains dispersed graphite at 0.8% of the diamond layer volume.
Pulverized bakelite was mixed with an aqueous nanodiamond suspension. The mixture was dispersed evenly in the emulsion, dried completely, and then mixed with ultrasonic vibration. The composite was sintered using the standard process for diamond wheels with polymer binders. Rings measuring 125 x 3 x 3 mm were produced for testing.
Microhardness response
Section titled “Microhardness response”Hardness was measured with a PMT-3 instrument at a 50 g load using a Vickers diamond pyramid with a 136° apex angle. The same load and indenter geometry applied to all measured compositions.
| Nanodiamond content | Vickers microhardness | Reported change from control |
|---|---|---|
| None, control | 78 HV | Baseline |
| 0.5 wt% | 91 HV | 16% increase |
| 1 wt% | 96 HV | 23% increase |
| 1.5 wt% | 93 HV | Not stated |
| 2 wt% | Not reported | Not reported |
At 0.5 wt%, hardness reached 91 HV, a 16% increase. At 1 wt%, it reached 96 HV, the largest measured gain. The 1.5 wt% specimen reached 93 HV, so the reported response did not rise continuously with nanodiamond content.
The authors recommend about 1 wt% of nanodiamond by binder mass. They also propose using the composition in standard diamond layers and expect hardness to improve while thermal conductivity remains constant. The paper does not report a thermal conductivity measurement for these specimens.
Grinding zone simulation
Section titled “Grinding zone simulation”The study used LS-DYNA to model the binder, diamond grain, and workpiece during grinding. The workflow covered geometry, finite element meshing, mesh parameterization, material behavior, contact interaction, loading, and result analysis.
The organic binder used a solid body model defined by elastic modulus, shear modulus, Poisson’s ratio, and density. The metal catalyst, metal coating, and workpiece used a plastic material model that extends Hooke’s law to von Mises plasticity. Figure 1 tracks stress against temperature for 63/50 grit. Figure 2 shows the stress distribution in the binder, grain, and metal phase at 150% grain concentration.
The authors identify temperature in the microcutting zone as a decisive factor in synthetic diamond failure and recommend controlling it along with force. The paper does not give numerical stress or temperature limits from the simulations. They therefore support a design method, not a measured operating window for a finished wheel.
Grain retention and metal coatings
Section titled “Grain retention and metal coatings”The paper proposes nanodiamond in both the resin binder and the nickel coating around synthetic diamond. For the coating route, a nanodiamond suspension was added during deposition of the second nickel layer and during subsequent layers. This approach modifies the existing chemical nickel plating process.
The paper reports that coating tests increased diamond wheel performance by 27% relative to a wheel using conventional nickel. It does not define the performance metric or provide the test conditions for that comparison. A separate conclusion states that replacing a manganese-rich alloy with a nickel alloy lowers failure probability under force and thermal load by 27%. These statements describe different comparisons and should not be treated as one result.
The simulations also indicate that the metal phase and its share of grain volume affect diamond grain efficiency. The calculations suggest that diamond concentration can fall below values used in serial production, although no percentage reduction is stated.
The conclusion gives grit-specific coating recommendations. It contrasts them with a conventional range reported as 56 to 100 wt%, but the percentage basis is not defined.
| Grain designation | Recommended coating value as reported |
|---|---|
| 50/40 to 80/63 | 175% to 200% |
| 100/80 to 160/125 | 150% to 175% |
| 200/160 to 400/315 | 125 wt% |
The table preserves the paper’s percentage values. The text calls them coating thickness, so the physical unit remains unclear. These values are recommendations derived from the study’s calculations, not values validated across multiple wheel builds.
Comparison with earlier polymer results
Section titled “Comparison with earlier polymer results”The paper places its binder data beside earlier nanodiamond polymer composites. In aromatic polyamide phenylon C-2, cited work increased abrasive wear resistance by 3.5 times. It also increased elastic modulus by 104.5 MPa and compressive yield strength by 6.5 MPa.
For fluoroelastomer, elastic modulus rose from 8.5 MPa to 92 MPa, while tensile strength rose from 15.7 MPa to 173 MPa. For the material labeled polysilicon, modulus rose from 19 MPa to 53 MPa, and tensile strength from 52 MPa to 154 MPa. For isoprene rubber, modulus rose from 7.7 MPa to 12.3 MPa, and tensile strength from 20.5 MPa to 28.2 MPa.
Those studies support the use of nanodiamond as a polymer modifier, but they used other matrices and did not test SFP-012A grinding wheels. The current result is narrower. It shows a hardness change in one phenolic binder under a single indentation condition, with no direct wear test on the modified bond.
Evidence limits and engineering implications
Section titled “Evidence limits and engineering implications”The hardness result supports about 1 wt% nanodiamond as a formulation candidate, but several design claims remain unresolved. The abstract lists 0.5, 1, and 2 wt% formulations, while the results include a 1.5 wt% specimen and give no hardness value for 2 wt%. The reported hardness results provide no replicate count, uncertainty, or statistical test.
No direct grain pullout, bonding strength, thermal conductivity, grinding force, surface finish, or wheel life result appears for the SFP-012A specimens. The LS-DYNA results lack published numerical limits, and the 27% coating comparison lacks a defined performance metric. Nanodiamond particle size and agglomeration measurements are also absent, although the mixing procedure was designed to limit agglomeration.
For wheel formulation development, about 1 wt% nanodiamond in SFP-012A is the formulation supported by the reported hardness data. Production changes require grain pullout and grinding tests because hardness alone does not establish retention or tool life. Each grit and coating pair should also be checked against the simulation inputs.
View Original Abstract
The article presents one of the options for developing scientifically based recommendations for choosing a rational combination of the strength of the binder, the size of the diamond grain, the concentration of diamond grains with the physical and mechanical properties of different types of binders in the manufacture of diamond grinding wheels. The conducted studies have shown the feasibility of using detonation nanodiamond powders as a modifier of the polymer binder. The introduction of nanopowder into the polymer leads to an increase in microhardness by 23%, and the recommended mass fraction of nanodiamond should be about 1% of the weight of the binder. It is possible to use such polymer compositions in the diamond layer of standard grades, which theoretically will increase their hardness due to constant thermal conductivity.
Advanced Thermal Simulation Service Diamond Heat Spreader Performance Analysis
View Specs →
High Concentration Quantum Grade Single Crystal Diamond
View Specs →
Single Crystal Cvd Diamond Plate
View Specs →Original source