Skip to content

Swelling‐Induced Stress‐Assisted Transfer of Nanodiamond Arrays With a PVA Carrier Tape for Conformal Bio‐Integrated Sensing and Labelling

FieldValue
JournalAdvanced Functional Materials
Published2026-05-22
AuthorsLuyao Zhang, L Wang, Xinhao Hu, Tai Nam Yip, Mingze Sun
DOI10.1002/adfm.76009

Water soluble tape moved HPHT nanodiamond arrays onto soft, hydrated surfaces with an efficiency above 98% in about 3 min at room temperature. The bilayer PVA carrier swelled during release and generated compressive stress that pressed the particles against the target. A composite tape that dissolved without swelling produced only 50% to 60% transfer efficiency, with gaps, particle loss, and visible residue. Carrier architecture, rather than water solubility alone, therefore controlled the transfer quality.

Swelling converts dissolution into release

Section titled “Swelling converts dissolution into release”

Commercial water soluble tapes had two structures. The bilayer tape used a pure PVA backing about 33 µm thick and a PVA adhesive layer about 20 µm thick. A composite tape embedded cellulose microfibers 10 to 50 µm long in the adhesive matrix.

During immersion, the bilayer backing began anisotropic swelling within 20 s. It expanded further and peeled itself from the substrate as one piece in roughly 60 s. The adhesive dissolved during this release.

Optical microscopy and traction force microscopy tracked fluorescent nanodiamond tracers on amine modified PDMS coated glass. At about 20 s, outward radial displacement indicated an ellipsoidal compressive stress field of 500 to 1000 Pa. By 30 s, the field dissipated and reversed as the gel detached.

The composite tape showed passive fragmentation and no significant particle displacement. Its cellulose fibers dispersed into the surrounding medium over several minutes.

Changing glycerol in the water from 0 to 50 wt% slowed tape swelling. The peak compressive stress fell from about 1000 to 100 Pa. Transfer efficiency fell from about 98% to 78% over the same series. The stress amplitude therefore tracked transfer yield in these tests.

The isolated PVA backing reached a swelling ratio of about 500% in the first 30 s. Its Young’s modulus fell from about 60 kPa to nearly 0.5 kPa during that interval. The backing changed from a stiff film into a deformable gel that accommodated surface topography.

Pattern fabrication and transfer measurement

Section titled “Pattern fabrication and transfer measurement”

The donor arrays used commercial HPHT nanodiamonds with native NV centers. The experiments describe a 100 to 200 nm donor population, while the experimental materials list gives the selected particle size as 150 nm.

Photolithography on silicon defined circles 4 µm in diameter with 10 µm spacing. Each circle contained 15 to 25 nanodiamonds. The patterned wafer was immersed in a 0.1 mg/mL nanodiamond solution for 30 min before resist removal.

Water soluble tape then picked up the array and contacted the target conformally. The assembly was immersed in deionized water for about 3 min. Gentle shaking accelerated separation, and partially detached PVA backing could be removed with tweezers without disrupting the pattern.

Transfer efficiency was the ratio of fluorescence intensity at the same sites before and after transfer. Images used 532 nm excitation and 650 to 800 nm emission collection. The analysis covered 400 to 600 circular sites per sample.

Substrate stiffness, curvature, and chemistry

Section titled “Substrate stiffness, curvature, and chemistry”

GelMA hydrogels with Young’s moduli of 18, 10, and 0.6 kPa tested the effect of compliance. Transfer efficiency fell from about 95% at 18 kPa to about 82% at 0.6 kPa. The decline became notable below 10 kPa.

The authors attributed this result to local deformation of softer gels. Deformation reduced the effective contact area and interfacial adhesion, which limited the number of particles that transferred.

PDMS cylinders tested curvature from 1 to 8 cm⁻¹, corresponding to radii of 0.125 to 1 cm. Efficiency stayed above 95% at every curvature. The flat control was highest, but the curved values varied nonmonotonically. The authors linked these variations to reduced contact area and uneven local stress.

Surface chemistry produced a clear ranking. Amino groups gave the highest efficiency, hydroxyl groups followed, and carboxyl groups gave the lowest. The authors attributed the amino result to electrostatic attraction and the carboxyl result to electrostatic repulsion. Hydroxyl surfaces supported hydrogen bonding.

The comparison used carboxyl functionalized and hydroxyl functionalized nanodiamonds on untreated and functionalized PDMS. Surface chemistry therefore belongs in transfer design, not only in later sensor functionalization.

Transfer across soft and curved interfaces

Section titled “Transfer across soft and curved interfaces”

A silicone hydrogel contact lens with about 50% water content and a Young’s modulus of about 0.5 MPa received a panda array. Its 4 µm circles had a 7 µm pitch and followed the lens curvature without visible cracks or aggregation.

On a gold neural probe, the authors transferred 4 µm circles at 10 µm spacing. The probe had a 500 µm base diameter and a 50 µm tip curvature. A PDMS micropillar test placed particles only on the tops of pillars 2 µm in diameter, 6 µm high, and spaced 4 µm apart.

The method also produced continuous arrays on human hair. Hair has a roughly 50 to 100 µm curvature radius, overlapping cuticle scales about 0.5 µm thick, and a lipid rich surface. A silicone prosthetic hand received sharply defined arrays.

A 2 inch text array on PET tested a larger flexible area. These results show that tape contact can follow soft curved surfaces and microscale structures. They do not establish sensor operation in tissue or long term biological stability.

The contact lens carried two identity functions. A 1250 µm QR code encoded a 31 character laboratory URL. The 31 bytes, or 248 bits, occupied about 1.250 mm², giving a reported storage density of about 198 bit/mm². A smartphone read the code in about 1 s at about 248 bit/s.

The second function used stochastic nanodiamond placement as a physical unclonable function. The authors made and transferred 100 QR codes. They imaged a 75 by 75 µm particle distribution in the bottom left alignment region, then reduced it to a 64 by 64 pixel binary code.

The average interdevice Hamming distance was 0.5049, close to the ideal random value of 0.5. The average intradevice distance was 0.0366 across 10 measurements per device, below the stated 10% threshold. The pairwise comparison also separated the 100 devices. The authors interpreted these values as strong device distinguishability, repeatability, and uniqueness.

A contact lens pattern remained intact for more than 1 month in room temperature water. Detachment occurred only after the hydrogel collapsed. Patterns on PDMS showed no deformation or detachment after 10,000 stretch cycles at 10% strain.

The authors state that commercial PVA tape can be customized in sizes larger than 2 inches. They also state that transfer efficiency does not depend on the overall tape or substrate size. The method was described as compatible with roll to roll manufacturing.

The reported large area example was 2 inches, so production scale processing was not demonstrated. Wafer scale patterning of 4 to 8 inches was limited by the initial silicon photolithography. The authors identify larger area nanodiamond self assembly or inkjet printing as possible routes around that step.

The main limitation is the gap between model surfaces and living environments. The authors expect transfer efficiency above 90% on simplified ex vivo substrates to decline in vivo. They cite ultra low stiffness, sharp curvature, mixed surface charges, and biofluids that cause ionic screening and changing wetting.

Long term adhesion has not been systematically validated under ions, proteins, pH changes, or mechanical motion. The authors call for water soluble tapes with swelling and adhesion adjusted by pH or ionic strength. They also propose direct patterning on the carrier to remove pickup from a rigid donor.

For device engineering, the paper supports using native NV HPHT nanodiamonds and selecting substrate chemistry before integration. Carrier swelling and surface charge must be tested with the intended tissue. Until in vivo adhesion and yield are measured, the demonstrated use remains ex vivo patterning and contact lens identity verification.

View Original Abstract

ABSTRACT The conformal integration of nitrogen‐vacancy (NV) center nanodiamond arrays onto soft, hydrated, curvilinear biological interfaces remains a fundamental challenge for in vivo quantum sensing and imaging. Conventional transfer techniques often fail due to reliance on high temperature, corrosive chemicals, or mechanical peeling, leading to pattern damage, low fidelity, or poor biocompatibility. Here, we report a transfer strategy utilizing polyvinyl alcohol (PVA) soluble tape that enabling rapid, residue‐free, high‐fidelity transfer of nanodiamond patterns onto diverse biointerfaces. The success of this method is rooted in a unique “hydrate‐soften‐expand‐self‐peel” mechanism of the PVA backing. In situ mechanical tracking reveals non‐uniform PVA swelling generates transient normal and shear stresses at the interface. These stresses delaminate the tape within 3 min at room temperature while promoting adhesion of nanodiamonds to the substrate. In contrast, conventional tapes undergo passive dissolution and collapse, causing residue contamination and reduced efficiency. Leveraging this mechanism, we achieve conformal patterning on ultra‐soft hydrogels (∼0.6 kPa) and highly curved bio‐surfaces (hair, 100 µm − 1 ). Additionally, we demonstrate a dual‐identity verification system integrating data storage and physical unclonable functions on a hydrogel contact lens. This work provides a versatile tool for bio‐interface engineering and a general framework for gentle, efficient transfer of functional nanomaterials.